Research on the Evolution Model of Grain Boundary Helium Bubbles in the Weld Heat-Affected Zone of Austenitic Stainless Steel After Irradiation.
Shaohua Yin, Zhiqiang Sun, Yingjie Chen, Zhaosheng Guo, Zhen Luo
School of Materials Science and Engineering, Tianjin University, Tianjin 300350, China. · Suzhou Nuclear Power Research Institute Co., Ltd., Suzhou 215004, China.
Key points
From the paper's conclusion- This study develops a multistage model to elucidate helium bubble evolution during welding, including nucleation, coalescence, high-temperature growth, and cooling-induced tensile stages, by quantitatively correlating bubble density/diameter with initial He concentration (0.2–20 appm (atomic parts per million)), peak temperature (1450 K, 1566 K, 1641 K, 1657 K), and stress (0–200 MPa).
Abstract
The weldability of neutron-irradiated austenitic stainless steels in pressurized water reactors (PWRs) deteriorates significantly due to helium accumulation at grain boundaries (GB) originating from nuclear transmutation reactions. This study develops a multistage model to elucidate helium bubble evolution during welding, including nucleation, coalescence, high-temperature growth, and cooling-induced tensile stages, by quantitatively correlating bubble density/diameter with initial He concentration (0.2-20 appm (atomic parts per million)), peak temperature (1450 K, 1566 K, 1641 K, 1657 K), and stress (0-200 MPa). Key results demonstrate that He concentration nonlinearly affects bubble growth (threefold diameter increase at 20 appm versus 0.2 appm during cooling), while temperature governs bubble kinetics with critical threshold behavior (>900 K) and tensile stress promotes cooling-stage expansion over the investigated stress range. Excessive welding heat input prematurely terminates coalescence, increasing final bubble density/diameter and promoting He-induced cracking, consistent with the reported morphology and order of magnitude of grain-boundary cavities. The model provides a theoretical framework for predicting He embrittlement and optimizing stress-modified welding techniques (e.g., auxiliary beam laser welding) for nuclear component repair.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of fabrication on microstructure and heat affected zone width in weldments of nuclear reactor pressure vessel steelMaterials & Design · 2026
- Grain boundary effects on surface modifications of tungsten under fusion-relevant helium plasma irradiation: Coarse-grained vs. Nano-grained microstructuresNuclear Fusion · 2026
- Surface Degradation of 08Cr16Ni11Mo3Ti Austenitic Steel Under Helium Plasma ExposureMetals · 2026
- Optimizing impact toughness in Q1100E steel welds via laser-arc hybrid welding energy ratio controlJournal of Materials Research and Technology · 2026
- Structural Integrity of Welded Pipe Joints Made of Creep–Resistant Steel P91 with Multiple Defects: Experimental Characterization and Engineering Critical AssessmentMetals · 2026
- Effects of temperature and welding heat input on abnormal grain growth in friction-stir welds of 2219 aluminum alloyMaterials & Design · 2025