Laser-Assisted Wafering of 4H-SiC: From Subsurface Modification and Crack Coalescence to Controlled Separation.
Zhiqiang Fan, Pengsen Zhang, Beichen Hu
School of Mechanics and Transportation Engineering, Northwestern Polytechnical University, Xi'an 710072, China. · The Second Research Institute of China Electronics Technology Group Corporation, Taiyuan 030024, China.
Key points
From the paper's conclusion- We connect nonlinear energy deposition, phase transformation and residual stress to crack nucleation, interaction and coalescence, and then assess mechanical and ultrasonic separation, polymer-assisted cold splitting, continuous-wave laser splitting, other thermal-stress routes, and chemical or hybrid release within a common fracture-mechanics framework.
Abstract
Laser-assisted wafering can reduce material consumption in silicon carbide (SiC) substrate manufacturing, but successful subsurface modification does not, by itself, guarantee controlled wafer release. This review treats 4H-SiC wafering as a two-step process comprising laser formation of a weakened subsurface layer, followed by assisted separation. We connect nonlinear energy deposition, phase transformation and residual stress to crack nucleation, interaction and coalescence, and then assess mechanical and ultrasonic separation, polymer-assisted cold splitting, continuous-wave laser splitting, other thermal-stress routes, and chemical or hybrid release within a common fracture-mechanics framework. Reported results show that crystallographic orientation, scan arrangement, crack coplanarity, acoustic coupling and liquid medium strongly affect separation. Nominal separation stress, residual stripping force and internally generated thermal stress are distinct metrics and should not be compared directly. Reported separation strengths span more than three orders of magnitude, from above 38 MPa to about 0.04 MPa, primarily because laser processing produces very different crack-network connectivity. As-split roughness ranges from about 0.16 to 6.5 µm and is governed mainly by the laser step and 4° off-cut geometry. Joint optimization of modification and separation, together with standardized reporting, is therefore essential for scalable low-loss wafering.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- A statistical framework for laser-induced subsurface modification and cracking in 4H-SiCScientific Reports · 2026
- Ultrafast laser-induced internal modifications and cross-scanning strategy for material-efficient 4H-SiC slicingOptics Express · 2025
- Femtosecond-laser wafer slicing of n-type 4 H-SiC in double-pulse MHz burst modeApplied Physics A · 2026
- High‐Efficiency Laser‐Assisted Manufacturing of Silicon Carbide Wafers and Components: A Critical ReviewEngineering Reports · 2026
- Laser Processing Methods in Precision Silicon Carbide Wafer Exfoliation: A ReviewJournal of Manufacturing and Materials Processing · 2025
- Advances in High-Efficiency, Low-Damage Polishing Technologies for Single-Crystal Silicon CarbideCrystals · 2026