Electrical Resistivity Response and Mesoscopic Simulation of Concrete Containing a Composite Low-Freezing-Point Powder Under Subzero Conditions.
Yangjun Deng, Xueqian Wang, Mingming Zhu, Dong Gao, Sheng Qiang
College of Water Conservancy and Hydropower Engineering, Hohai University, Nanjing 210098, China. · Liaoning Provincial Water Conservancy and Hydropower Survey, Design and Research Institute Co., Ltd., Shenyang 110002, China.
Key points
From the paper's conclusion- Considering both delayed apparent freezing onset and strength retention, 4%CLFP was identified as a suitable dosage for balancing these two indicators under the tested conditions.
Abstract
Abrupt temperature drops during cold waves pose a threat to early-age concrete in cold regions. This study combined electrical resistivity monitoring, compressive strength testing, and mesoscopic electrical modeling to investigate the performance of concrete containing a composite low-freezing-point powder (CLFP). CLFP comprised calcium nitrate tetrahydrate and sodium nitrite at a mass ratio of 3:1. Five dosages of 0%, 2%, 4%, 6%, and 8% were investigated, and the specimens were cured at -20 °C for 3 d before being transferred to 20 °C. A random-aggregate model was used to link experimentally measured time-dependent mortar conductivity to the overall electrical resistivity of concrete, and the electrical responses were evaluated alongside subsequent strength development. All mixtures exhibited three resistivity stages: slow increase, rapid rise, and stabilization. Increasing the CLFP dosage delayed the resistivity-derived apparent freezing onset by up to 0.43 h and reduced the stabilized resistivity by 29.96%. After 28 d of subsequent curing at 20 °C, the 2% CLFP mixture achieved the highest compressive strength of 37.6 MPa, approximately 7.1% higher than the reference value of 35.1 MPa. The 4%CLFP mixture reached 35.4 MPa, whereas the 6% and 8% mixtures reached only 24.1 MPa and 25.3 MPa, respectively. The model reproduced the decrease in stabilized resistivity with increasing CLFP dosage, with relative errors of 1.5-8.4% for the 0-6%CLFP mixtures and 18.2% for the 8% mixture. Considering both delayed apparent freezing onset and strength retention, 4%CLFP was identified as a suitable dosage for balancing these two indicators under the tested conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Stabilized electrical conductivity in nano-engineered ultra-high performance concrete under prolonged freezing exposure: Nano-reinforcement and cryo-induced water migration mechanismConstruction and Building Materials · 2026
- Experimental Investigation on Flexural Behavior of Desert Sand Concrete Beams Subjected to Freeze–Thaw CyclesMaterials · 2026
- Freeze-Thaw Damage Evolution of PVA-Fly Ash-Slag Composite Concrete and Low-Dimensional Mapping of Weibull Characteristic Parameters.Materials (Basel, Switzerland) · 2026
- Strength Evolution and Promotion for Ultra-Early-Age Concrete Under Low TemperatureMaterials · 2026
- Numerical Simulation and Experimental Validation of the Resistance of Recycled Aggregate Concrete to Chloride Penetration Under Freeze-Thaw Cycles.Materials (Basel, Switzerland) · 2026
- Pressed Cement-Free and Low-Cement Materials Based on Recycled Concrete Powder.Materials (Basel, Switzerland) · 2026