The Effect of Y, La, Lu, and K on the Segregation and Cohesion of Tungsten Grain Boundaries.
Mingyu Wu, Chengzhen Miao, Nanxi Zhao, Kaige Shen, Yujuan Zhang, Yan Zhao, Yanfei Qi, Changchun Ge
Institute of Nuclear Materials, School of Materials Science and Engineering, University of Science and Technology Beijing (USTB), Beijing 100083, China. · College of Metallurgy and Energy, North China University of Science and Technology (NCST), Tangshan 063210, China.
Key points
From the paper's conclusion- We have systematically analyzed the solution and aggregation characteristics of yttrium (Y), lanthanum (La), lutetium (Lu) and potassium (K) on symmetrically inclined tungsten (W) grain boundary (GB) Ʃ5(310)/[001] by first principles calculation.
Abstract
We have systematically analyzed the solution and aggregation characteristics of yttrium (Y), lanthanum (La), lutetium (Lu) and potassium (K) on symmetrically inclined tungsten (W) grain boundary (GB) Ʃ5(310)/[001] by first principles calculation. Furthermore, the influence mechanism of Y, La Lu and K on the strength of W GB was analyzed. K/La and Y/Lu exhibit two different evolution characteristics in the W GB region. The calculation results show that Y/Lu preferentially occupies the substitution site (V0) on the W GB plane, and the solution energy of Y/Lu at the substitution site increases with distance from the W GB plane. However, the most stable occupation sites of La/K in the W GB region are the sites (V1) nearest to the W GB plane. The electronic structure analysis showed that the segregation energies of Y, La Lu and K on the W GB were positively correlated with the number of electron transfer. The existence of K/La in the W GB region promotes the dissolution of subsequent atoms, while the existence of Y/Lu atoms has little effect on the dissolution of subsequent atoms. In terms of mechanical properties, the addition of alloying elements significantly improves the fracture energy of W GB, and the Y and Lu effectively increase the fracture energy to 5.602 J/m2 and 5.687 J/m2, which is higher than the 5.185 J/m2 of clean W GB. This strengthening mechanism is mainly attributed to the strong metal bond between W-Y and W-Lu. Although the fracture energy of La and K is also higher than that of clean W GB-5.465 J/m2 and 5.335 J/m2, respectively-the strength improvement mainly depends on the action of La-La and K-K metal bonds.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- A GRACE Interatomic Potential for W--Ta Systems: Application to Ta Segregation and Pinning of Shear-Coupled Grain-Boundary MigrationarXiv · 2026
- Microstructural evolution and strengthening mechanisms of gas tungsten arc welded nickel-based superalloy joints processed by laser powder bed fusion: Effects of welding direction and heat inputJournal of Materials Processing Technology · 2025
- Alloying effects on the interface cohesion of grain boundaries in the Ni--Fe--Cr systemarXiv · 2026
- Making high-W-content Ta-W alloys ductile via minor alloying of HfMaterials Research Letters · 2025
- Grain boundary effects on surface modifications of tungsten under fusion-relevant helium plasma irradiation: Coarse-grained vs. Nano-grained microstructuresNuclear Fusion · 2026
- The defect chemistry of the Σ5(310)[001] grain boundary in lanthanide doped uranium dioxide, and its implications for the dissolution of spent nuclear fuelJournal of Physics: Energy · 2026