Transient Liquid Phase Bonding Using Sputtered Cu/Sn Multilayers.
Dong-Yurl Yu, Junhyuk Son, Yun-Chan Kim, Yong-Ho Ko, Tae-Young Lee, So-Jeong Lee, Dongjin Byun, Junghwan Bang
Advanced Packaging Integration Center, Korea Institute of Industrial Technology, 156 Gaetbeol-ro, Yeonsu-gu, Incheon 21999, Republic of Korea. · Center for Cooperative Research Facilities, Tech University of Korea, 65 Emtibeuibukro-ro, Siheung-si 15119, Republic of Korea.
Key points
From the paper's conclusion- In this study, transient liquid phase (TLP) joints were fabricated using sputtered Cu/Sn multilayers, and their mechanical performance was evaluated through isothermal aging at 175 °C for up to 500 h and die-shear testing.
Abstract
Power electronic modules require bonding materials capable of maintaining high reliability during high-temperature operation. In this study, transient liquid phase (TLP) joints were fabricated using sputtered Cu/Sn multilayers, and their mechanical performance was evaluated through isothermal aging at 175 °C for up to 500 h and die-shear testing. The effects of the initial Cu/Sn multilayer configuration on interfacial microstructural evolution and shear strength were systematically investigated. In the as-bonded state, Cu6Sn5 and Cu3Sn intermetallic compounds (IMCs) were formed in the three primary configurations, while localized cracking was observed in an additional 7layer/7layer configuration examined only in the as-bonded state. During aging, the Cu6Sn5 to Cu3Sn transformation strongly depended on the initial multilayer configuration, although the three primary configurations were completely transformed into Cu3Sn after 500 h. A comparative kinetic analysis suggested a higher apparent Cu3Sn growth rate for the 5layer/5layer configuration, although this trend was derived from a limited number of aging time points. The 5layer/5layer joints exhibited the highest initial shear strength, which was attributed to the presence of an island-shaped Cu3Sn region within the bonding layer. After 500 h of aging, however, the 3layer joints exhibited the highest shear strength, consistent with their lower interfacial void fraction, whereas the 5layer/5layer joints exhibited the greatest void accumulation. These results demonstrate that the initial Cu/Sn multilayer architecture plays an important role in IMC transformation, interfacial void evolution, and shear strength evolution during isothermal aging at 175 °C. Therefore, controlling the Cu/Sn multilayer configuration provides a potential approach for tailoring the microstructure and mechanical performance of Cu3Sn joints under the investigated aging conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Overview of Low-Temperature Sn-Bi and Sn-Zn Solder Systems and Cu Interfacial Reliability for Advanced Electronic Packaging.Micromachines · 2026
- Interfacial Reaction and Shear Behavior of Sn-19Bi-19In Solder Joints on an ENEPIG Surface Finish During Isothermal Aging.Micromachines · 2026
- A novel sandwich-structured interlayer enabled high-performance GH4169D TLP bonded jointScience and Technology of Welding & Joining · 2025
- Thermal Input-Driven Interfacial Phase Evolution and Mechanical Reliability of Zn-15Al Brazed Cu/Al JointsCrystals · 2026
- Transient Simulation and Experimental Study of Intermetallic Formation using Sn/Cu/Sn Preforms in Inductive Chip-Level Solid-Liquid Interdiffusion Bonding for Microelectronics ApplicationsJournal of Materials Engineering and Performance · 2026
- Low-Temperature, Large-Area Sinter-Bonding of Dendritic Cu Paste for Substrate-to-Base-Plate JointsMetals · 2026