Effect of Extrusion Ratio on Microstructure and Mechanical Properties of 7A85 Aluminum Alloy.
Zhengbin Ma, Wenli Gao
School of Materials Science and Engineering, Hunan University, Changsha 410082, China.
Key points
From the paper's conclusion- This work provides guidance for optimizing the extrusion process parameters of 7A85 aluminum alloy.
Abstract
The extrusion ratio strongly influences the deformation behavior and final properties of aluminum alloy extrusions. In this study, the effects of extrusion ratio (13, 16, 20, and 26) on the microstructure and mechanical properties of 7A85 aluminum alloy were investigated by tensile testing, hardness and electrical conductivity measurements, EBSD characterization, and DEFORM-3D finite element simulation. The results show that the sample with an extrusion ratio of 13 has the finest recrystallized grains (5.73 μm) and the highest average misorientation angle (26.25°), indicating a relatively high degree of recrystallization. In contrast, although the sample with an extrusion ratio of 20 exhibited a mixed grain structure (a mixture of fine and coarse grains) and incomplete recrystallization, it achieved the highest as-extruded tensile strength (502 MPa). The strength degradation of the sample with an extrusion ratio of 26 is due to excessive recovery and grain coarsening. After T6 heat treatment, the strength difference between samples with different extrusion ratios was basically eliminated (~690-697 MPa). Combined with the simulation results under different extrusion ratios, the temperature field and material flow field in the extrusion process were analyzed, and the deformation and recrystallization mechanisms were deeply understood. These results indicate that the intermediate extrusion ratio can provide the best balance for the as-extruded material's strength, and the T6 aging response is relatively insensitive to the extrusion ratio. However, fine and uniform recrystallized grains are more conducive to a stable aging response. This work provides guidance for optimizing the extrusion process parameters of 7A85 aluminum alloy.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Role of Er element and two-stage heat treatment in a rheo-extruded Al–Sc–Zr alloy: Balance strength and electrical conductivityMaterials & Design · 2025
- Influence of extrusion preheating temperature and aging strategy on precipitation and performance of Al–Sc–Zr conductor alloysMaterials Today Communications · 2026
- High strength-ductility synergy achieved in low-alloyed Mg alloys via hyper-substructure introduction through upsetting-assisted asymmetric extrusionJournal of Magnesium and Alloys · 2026
- Correlation between microstructure and mechanical properties in A356 aluminum alloyMATEC Web of Conferences · 2026
- Homogenization-free fabrication of a high-strength ductile melt-impact-deposited 7055 Al alloy via extrusion-assisted defect healing and Al3Sc-based/η′ precipitation synergyJournal of Materials Research and Technology · 2026
- Cryogenic rolling synergistically enhances mechanical properties and electrical conductivity of an Al-0.7Mg-0.4Si-0.1Fe alloyJournal of Materials Research and Technology · 2025