Comparative Electrochemical Noise Characterization of Ti-CP2, Ti-6Al-2Sn-4Zr-2Mo, and Ti-6Al-4V in Ringer's Solution Using Statistical and Hilbert-Huang Analyses.
Citlalli Gaona-Tiburcio, Erick Maldonado-Bandala, Jesús Manuel Jáquez-Muñoz, Demetrio Nieves-Mendoza, Ce Tochtli Méndez-Ramírez, Bruno Almeraya-Gaona, Laura Landa-Ruiz, Brenda Baltazar-Garcia,
Centro de Investigación e Innovación en Ingeniería Aeronáutica (CIIIA)/Facultad de Medicina, Facultad de Ingenieria Mecanica y Eléctrica, Universidad Autónoma de Nuevo León, San Nicolás de los Garza 66455, Mexico. · Facultad de Ingeniería Civil, Universidad Veracruzana, Xalapa 91000, Mexico.
Key points
From the paper's conclusion- This study comparatively evaluated the electrochemical behavior of Ti-CP2, Ti-6Al-2Sn-4Zr-2Mo, and Ti-6Al-4V in Ringer’s solution using electrochemical noise (EN), empirical mode decomposition (EMD), Hilbert–Huang Transform (HHT), and scanning electron microscope/Energy-dispersive X-ray spectroscopy (EDS) SEM/EDS characterization.
Abstract
Titanium and its alloys are widely used in biomedical applications because of their favorable mechanical properties, biocompatibility, and corrosion resistance. This study comparatively evaluated the electrochemical behavior of Ti-CP2, Ti-6Al-2Sn-4Zr-2Mo, and Ti-6Al-4V in Ringer's solution using electrochemical noise (EN), empirical mode decomposition (EMD), Hilbert-Huang Transform (HHT), and scanning electron microscope/Energy-dispersive X-ray spectroscopy (EDS) SEM/EDS characterization. Statistical EN analysis revealed marked differences among the investigated materials. Ti-6Al-2Sn-4Zr-2Mo exhibited the highest noise resistance (45,412 ± 57 Ω·cm2), followed by Ti-6Al-4V (11,784 ± 39 Ω·cm2) and Ti-CP2 (4114 ± 45 Ω·cm2), whereas relatively low localization index values were obtained for all three materials (0.02634-0.06). EMD revealed four, five, and six intrinsic mode functions for Ti-CP2, Ti-6Al-2Sn-4Zr-2Mo, and Ti-6Al-4V, respectively. Hilbert time-frequency-amplitude analysis further demonstrated distinct temporal and frequency distributions of the electrochemical fluctuations, with Ti-6Al-4V exhibiting the broadest and most persistent distribution of transient activity. SEM/EDS revealed localized post-exposure compositional heterogeneity and different degrees of accumulation of electrolyte-derived species but was not interpreted as direct evidence of passive-film chemistry or integrity. Overall, the combined statistical EN, EMD, Hilbert time-frequency, and SEM/EDS results demonstrate distinct passive electrochemical responses among the three titanium materials, with Ti-6Al-2Sn-4Zr-2Mo exhibiting the highest resistance to electrochemical fluctuations under the investigated conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Evaluation of the Influence of Tantalum on the Microstructural, Mechanical and Electrochemical Properties of Ti-Mo-Zr-xTa Alloys for Use in Biomedical Devices.Journal of functional biomaterials · 2026
- Comparative Electrochemical and Time-Dependent Passivation Behavior of Titanium Materials with Different Phase Constitutions in 3.5 wt.% NaCl at 37 °CMetals · 2026
- Corrosion Behavior of Ti-Nb-Zr-Si Alloy after One-Year Exposure to Simulated Inflammatory Conditions.ACS omega · 2026
- Effect of Annealing Temperature on Electrochemical Behavior of Commercially Pure Titanium with α′-Martensite in Solution Containing Fluoride IonsArchives of Dentistry · 2026
- Titanium Alloys at the Interface of Electronics and Biomedicine: A Review of Functional Properties and ApplicationsElectronic Materials · 2026
- Electrochemical Activity and Corrosion Behavior of Ultrafine-Grained Ti-xMo Alloys Processed via Powder MetallurgyMaterials · 2026