Interfacial Characteristics and Metallurgical Mechanism of Sapphire/TC4 Alloy Joints Produced by Femtosecond Laser Welding.
Yue Zhao, Xiaoyang Wang, Jiangtao Liang, Sen Huang, Yinghao Cui, Quanqi Zuo, Shirun Guo, Lujun Cui
School of Intelligent Mechatronic Engineering, Zhongyuan University of Technology, Zhengzhou 451191, China. · Shougang Research Institute of Technology, Shougang Group Co., Ltd., Beijing 100043, China.
Key points
From the paper's conclusion- The results revealed that the femtosecond laser induced transient high temperatures, elemental intermixing, and interfacial metallurgical reactions at the sapphire/TC4 alloy interface, producing an interfacial compositional transition zone with a maximum measured width of 5.72 μm after rapid cooling.
Abstract
Femtosecond laser welding of sapphire to TC4 (Ti-6Al-4V) alloy was conducted under atmospheric conditions, and the interfacial characteristics, metallurgical reaction mechanism, and the effect of laser power on joint strengthening were systematically investigated. The results revealed that the femtosecond laser induced transient high temperatures, elemental intermixing, and interfacial metallurgical reactions at the sapphire/TC4 alloy interface, producing an interfacial compositional transition zone with a maximum measured width of 5.72 μm after rapid cooling. Reaction products including TiO, TiO2, and Al3Ti were identified by XRD, while EDS revealed interfacial redistribution of Ti, Al, and O. At a laser power of 8.4 W, the joint exhibited a relatively flat interfacial morphology and a lower apparent shear strength than that at 12.4 W. The highest mean apparent shear strength of 51.55 MPa was obtained at 12.4 W, which was associated with the characteristic wavy interfacial morphology that promoted crack deflection and energy dissipation. At 16.6 W, interconnected microcracks formed near the interface and within the sapphire substrate due to excessive heat input and thermal mismatch, and the apparent shear strength decreased to a level statistically comparable to that at 8.4 W.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Tailoring sapphire–invar welds using burst femtosecond laserLight Advanced Manufacturing · 2025
- Femtosecond Laser Welding of N-BK7 Glass: From In-Volume Modification to Large-Scale, High-Strength JoiningMicromachines · 2026
- Femtosecond laser welding of non-optical-contact ceramic and fused silicaOptics Letters · 2025
- Ultrafast laser direct welding of sapphire and Invar under non-optical contact conditions with white-light-interferometric gap measurementOptics Express · 2025
- Process Parameter Optimization and Crack Formation Mechanism of Femtosecond Laser Welding of Fused Silica/6061 Aluminum Alloy.Nanomaterials (Basel, Switzerland) · 2026
- Plasma behaviors and welding property control in non-optical contact metal-glass laser welding.Applied optics · 2026