From the paper's conclusion- In this work, soft magnetic coatings were fabricated from Fe-Ni-Cr (1J38) alloy powders via high-velocity oxygen-fuel (HVOF) spraying.
Abstract
In this work, soft magnetic coatings were fabricated from Fe-Ni-Cr (1J38) alloy powders via high-velocity oxygen-fuel (HVOF) spraying. The microstructural features and intrinsic magnetic properties were characterized using scanning electron microscopy (SEM), X-ray diffraction (XRD), and a background signal stripping algorithm. Furthermore, the microstructural defects and magnetic degradation characteristics of coatings with varying thicknesses were comparatively analyzed. The results indicate that while the HVOF deposits exhibit exceptional density, the rapid quenching process inevitably induces oxygen-rich inter-splat boundary networks and residual stresses within the coatings. XRD analysis reveals no significant macroscopic oxidation or phase transformation during deposition, demonstrating a high-fidelity retention of the original face-centered cubic (FCC) lattice structure of the feedstock alloy. Magnetic measurements, upon the precise elimination of substrate background interference, reveal a distinct wasp-waisted magnetization distortion at low magnetic fields. This phenomenon can be attributed to the asynchronous magnetization response between the easily reversed, unoxidized soft-magnetic splat cores and the high-barrier boundary pinning networks (composed of inter-splat oxide interlayers and localized high-stress concentrations) within the coating. Compared to the thicker deposits (0.5 mm), the thinner coatings (0.3 mm) exhibit superior magnetic performance, characterized by a lower intrinsic coercivity. This degradation in thicker coatings is ascribed to the substantial accumulation of macroscopic residual stresses during deposition, which exert a stronger pinning effect on magnetic domain wall motion.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of NiFe2O4 Phase and tribological properties on Vacuum plasma spray Cr3C2+25NiCr coating ER 2205 - 66Co26Cr5WC filler high-strength alloy plate fabricated by wire arc additive manufacturing processJournal of the Taiwan Institute of Chemical Engineers · 2025
- In-Depth Microstructural Analysis of High-Performance Nickel Chromium Coating with Complex CompositionJournal of Thermal Spray Technology · 2025
- Influence of HVOF Processing Parameters on the Amorphous Fraction and Properties of FeCrMoBC CoatingsCoatings · 2026
- Effect of Annealing Temperature on Microstructure and Mechanical Properties of (NiCr-Cr3C2)/NiCr Gradient Composite Coatings Prepared by HVOF TechnologyCoatings · 2026
- Effect of Deposition Defects on the Wear and Corrosion Resistance Behavior of HVOF-Sprayed 304 Stainless Steel CoatingsCoatings · 2026
- Parametric investigation of air jet erosion behavior of CrB₂ - and TiC-reinforced high velocity oxy-fuel (HVOF) sprayed WC–12Co coatingsIronmaking & Steelmaking Processes Products and Applications · 2026