Amorphous Ribbon Brazing Filler Metals: Selection Criteria, Glass Formation, and Transient Liquid Phase Bonding.
Alexander Ivannikov, Sofya Terekhova, Alexey Suchkov, Ivan Fedotov, Nikita Popov, Ivan Klyushin, Pavel Morokhov, Oleg Sevryukov
Department of Materials Science, National Research Nuclear University MEPhI (Moscow Engineering Physics Institute), Kashirskoe Shosse 31, 115409 Moscow, Russia.
Key points
From the paper's conclusion- This selection is no accident: to become the basis of a commercial filler metal, an amorphous alloy must simultaneously satisfy five criteria (C1-C5) of brazing temperature, glass formation, base-material compatibility, ribbon manufacturability, and cost and safety, which are formulated here as a single cross-system checklist with operational thresholds.
Abstract
Amorphous ribbon brazing filler metals produced by rapid melt quenching form a distinct class of high-temperature brazing materials; a few ductile microcrystalline ribbons are treated as boundary cases. This review systematizes the four industrial families of such fillers: copper-phosphorus (Cu-Ni-Sn-P), titanium (Ti-Cu-Ni, Ti-Zr-Cu-Ni(-Be)), zirconium (Zr-Ti-Cu-Ni, Zr-Cu-Fe-Be), and nickel-metalloid (Ni-Cr-Si-B, Ni-Cr-P) alloys, together with the closely allied iron-based fillers. This selection is no accident: to become the basis of a commercial filler metal, an amorphous alloy must simultaneously satisfy five criteria (C1-C5) of brazing temperature, glass formation, base-material compatibility, ribbon manufacturability, and cost and safety, which are formulated here as a single cross-system checklist with operational thresholds. The class itself exists because in deep eutectics, the depressant and glass-former functions can coincide. Transient liquid phase (TLP) bonding, for which the thin homogeneous ribbon is a particularly suitable carrier, runs through the review as a unifying thread. The structural heredity of the ribbon-derived melt and the complementarity of the families by base material are discussed; ductile silver and aluminum fillers serve as a negative control delineating the boundary of the class, and the criteria are applied predictively to compare the families and to select a filler metal for a specific task.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Single-Step Induction Brazing of Ceramic–Metal Hybrid Joints: Tailoring Zirconium Content for Microstructure and Mechanical PerformanceApplied Sciences · 2026
- Solidification‐Derived Intermetallic Architectures in Heat‐Resistant Aluminum Alloys: A ReviewAdvanced Engineering Materials · 2026
- A novel sandwich-structured interlayer enabled high-performance GH4169D TLP bonded jointScience and Technology of Welding & Joining · 2025
- Laser powder bed fusion of Cu/17-4 PH multi-material system: Microstructural evolution and structure-property relationshipsJournal of Materials Research and Technology · 2026
- Aluminum- and Zirconium-Based Amorphous Alloys: A Comparative Review of Glass Formation, Crystallization, Mechanical Behavior, Processing and ApplicationsEntropic and Disordered Matter · 2026
- Additive manufacturing of Ti2AlNb alloys: A review of process, microstructure, property relationshipsMaterials Science and Engineering R Reports · 2026