Materials (Basel, Switzerland)

Valorisation of Pre- and Post-Consumer Cotton, Viscose and Bast-Fibre Textile Waste into Sodium Carboxymethyl Cellulose: A Comprehensive Study of Feedstock Type, Synthesis Route and Product Quality.

Marcin Małek, Norbert Lipka, Marcin Szeliga, Monika Tabor

Faculty of Civil Engineering and Geodesy, Military University of Technology (Wojskowa Akademia Techniczna), gen. Sylwestra Kaliskiego 2, 00-908 Warsaw, Poland. · CMC S.A., Weteranów 12, 03-172 Warsaw, Poland.

Key points

From the paper's conclusion
  • The results demonstrate laboratory-scale conversion of mechanically shredded textile waste into technical-grade CMC spanning a broad viscosity range.

Abstract

Sodium carboxymethyl cellulose (Na-CMC) is among the most widely used water-soluble cellulose ethers, yet its industrial production still relies largely on virgin cotton linters and wood pulp. In this work, we systematically converted a broad panel of cellulose-bearing textile wastes-reference fabrics, pre-consumer sewing-room clippings and post-consumer garments made of cotton, viscose, flax, jute and their blends-into Na-CMC through heterogeneous alkalisation and etherification in an isopropanol-water medium. Five synthesis routes were compared, including single-step, stepwise-reagent, hydrogen peroxide (H2O2) bleaching/degrading, cross-linking (dichloroacetic acid) and sodium monochloroacetate (MCA-Na) variants. Fifty-five separate batch syntheses were characterised for degree of substitution (DS), 2% apparent viscosity, active-substance purity, pH and residual moisture. The mean DS was 0.48 ± 0.07 and did not differ significantly among feedstock classes; used garments yielded similar mean substitution levels to reference fabrics in the statistical comparison. Product purity, in contrast, was lower on average for post-consumer material (71.9%) than for reference fabrics (75.9%), with a broader post-consumer distribution. scanning electron microscopy/energy-dispersive X-ray spectroscopy (SEM/EDS) examination of the feedstocks matched this trend, showing frayed, contaminated post-consumer fibres with sulfur signals and locally elevated aluminium on the fibre surface, which were not observed on the smooth pre-consumer cotton. DS showed moderate positive correlations with purity and log-viscosity. Apparent viscosities spanned four orders of magnitude (2.5-23,100 mPa·s), enabling a single, tunable process to deliver both low- and high-viscosity grades. The moderate DS (reagent efficiency ≈ 42%) is consistent with the monochloroacetate charge and reagent losses to hydrolysis rather than with the textile origin of the cellulose, and hydrogen peroxide lowered viscosity to 2.5-30 mPa·s without a significant loss of substitution. The results demonstrate laboratory-scale conversion of mechanically shredded textile waste into technical-grade CMC spanning a broad viscosity range.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers