Materials (Basel, Switzerland)

Microstructural, Mechanical, and Adhesive Characterization of Nanofluorapatite-Modified Orthodontic Resin-Modified Glass Ionomer Cement: A Preliminary In Vitro Study.

Wojciech Dobrzyński, Anna Nikodem, Joanna Weżgowiec, Rafał J Wiglusz, Marcin Mikulewicz

Department of Dentofacial Orthopedics and Orthodontics, Division of Facial Abnormalities, Faculty of Dentistry, Wroclaw Medical University, Krakowska 26, 50-425 Wroclaw, Poland. · Department of Mechanics, Materials and Biomedical Engineering, Faculty of Mechanical Engineering, Wrocław University of Science and Technology, Łukasiewicza 7/9, 50-371 Wroclaw, Poland.

Preclinical

Key points

From the paper's conclusion
  • Overall, nFAp incorporation improved resistance to debonding without a corresponding change in local indentation properties, with 2 wt.% nFAp showing the most favorable descriptive overall mechanical profile among the tested formulations.

Abstract

Nanofluorapatite (nFAp) was incorporated into GC Fuji Ortho LC resin-modified glass ionomer cement at 2 wt.% and 5 wt.% to assess its influence on microstructure, local mechanical properties, and orthodontic bond strength. The unmodified and nFAp-modified formulations were characterized by micro-computed tomography, backscattered-electron scanning electron microscopy with energy-dispersive X-ray spectroscopy (BSE-SEM/EDS), instrumented Vickers indentation, shear bond strength (SBS) testing, Weibull analysis, and Adhesive Remnant Index (ARI) scoring after debonding of orthodontic molar tubes bonded to human molars. Micro-CT showed higher porosity and resolved pore number density after nFAp incorporation, while pore dimensions changed only modestly. BSE-SEM/EDS showed microscale compositional heterogeneity and a markedly higher Ca signal in the modified materials. Indentation hardness and modulus did not differ significantly among groups. Mean SBS increased from 12.47 ± 2.41 MPa in the reference group to 17.31 ± 2.34 MPa and 16.66 ± 2.60 MPa for 2 wt.% and 5 wt.% nFAp, respectively; both modified groups differed significantly from the reference group but not from each other. ARI distributions were similar among groups. Overall, nFAp incorporation improved resistance to debonding without a corresponding change in local indentation properties, with 2 wt.% nFAp showing the most favorable descriptive overall mechanical profile among the tested formulations.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers