Influence of Fine and Coarse Waste Tyre Rubber Aggregates on the Workability, Mechanical Properties and Rubber-Paste Interface of Concrete: An SEM/EDX Study.
Marouan Bajbouji, Khalid Rkha Chaham, Saad Bensallam, Abdelmalek Goumih, Imane Mahboub
Laboratoire Sciences de l'Eau, Biotechnologies Microbiennes et Durabilité des Ressources Naturelles, Département de Géologie, Faculté des Sciences Semlalia, Université Cadi Ayyad, Marrakech 40000, Morocco. · Department of Roadways and Transport (PCT), École Hassania des Travaux Publics (EHTP), Km 7, Route d'El Jadida, B.P. 8108, Casablanca 20250, Morocco.
Key points
From the paper's conclusion- Compressive strength decreased by 8.5% with 10 vol. % fine rubber replacement and by 81.8% with 50 vol. % coarse rubber replacement, with coarse rubber consistently resulting in greater strength loss at all levels.
Abstract
Waste tyre rubber serves as a cost-effective aggregate substitute. The elemental-level interfacial mechanisms underlying the associated strength reduction remain insufficiently characterised. In this study, eleven concrete mixes were evaluated, with fine-rubber (2.5-5 mm) replacing river sand and coarse-rubber (5-20 mm) replacing crushed limestone, each at 10, 20, 30, 40 and 50% by volume. Cement content was maintained at 400 kg/m3 and the water-to-cement ratio at 0.45. Workability, hardened density, and 28-day compressive and flexural strengths were measured in accordance with Moroccan Standards (NM), which are aligned with the European Standards (EN). Scanning electron microscopy with energy-dispersive X-ray (SEM/EDX) microanalysis was conducted on six mixes to characterise the rubber-paste interfacial transition zone (ITZ). Compressive strength decreased by 8.5% with 10 vol. % fine rubber replacement and by 81.8% with 50 vol. % coarse rubber replacement, with coarse rubber consistently resulting in greater strength loss at all levels. Every qualifying paste-side field in the rubberised mixes returned a Ca/Si ratio above the reference bulk-paste value of 1.24, reaching 8.09, indicating portlandite accumulation at the hydrophobic rubber surface. Sulphur and zinc, introduced during vulcanisation, confirmed these regions as rubber rather than cement paste. The apparent debonding-zone width at the fracture surface increased from 10-25 µm to 100-200 µm and scaled with particle size, consistent with a flaw-size effect rather than with total interfacial area. Preliminary guidance on mix selection based on 28-day mechanical performance is proposed.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructural properties of ordinary concrete mixed with rubber and plastic waste under aggressive environmental conditions: A full‐factorial design studyStructural Concrete · 2026
- Quantitative characterization of crumb rubber concrete interfacial transition zone based on microscopic test methodConstruction and Building Materials · 2025
- Surface treatments of waste tyres for sustainable concrete production: A performance, environmental and cost-based reviewConstruction and Building Materials · 2026
- Rubberized Geopolymer Concrete for Sustainable Construction: A Critical Review of Interface Engineering, Performance Trade-Offs, Durability, and Environmental ImpactsSustainability · 2026
- Strength reduction of crumb rubber concrete: microstructures and mesoscale modellingInternational Journal of Mechanical Sciences · 2025
- Experimental Investigations on the Flexural Responses of Reinforced Rubberized Concrete Beams with High Rubber Contents and Longitudinal Reinforcement Ratios.Materials (Basel, Switzerland) · 2026