Toughening Mechanism and Nonlinear Water-to-Binder Ratio Effects in Multi-Scale Steel Fiber-Calcium Carbonate Whisker Reinforced Concrete.
Jiyang Wang, Xianmo Xu, Xiaoyao Ren, Lingbo Wang, Xiaohua Ji, Bocheng Xie, Pinghuai Zhou
Institute of Advanced Engineering Structures, Zhejiang University, Hangzhou 310058, China. · Zhejiang Communications Construction Group Co., Ltd., Hangzhou 310007, China.
Key points
From the paper's conclusion- Together, these actions established a hierarchical toughening mechanism spanning microdefect regulation and macrocrack bridging, transforming abrupt brittle fracture into progressive cracking while sustaining structural integrity.
Abstract
The toughening efficiency of multiscale fibers is strongly coupled with the matrix state, yet how the water-to-binder (w/b) ratio shifts the governing reinforcement mechanism remains unclear. Two w/b regimes representing distinct matrix conditions were therefore incorporated into a three-factor, four-level orthogonal design, with water, steel-fiber, and calcium carbonate whisker dosages as variables. Compressive, flexural, and direct tensile strengths, together with failure characteristics, were evaluated to track the transition in mechanical response across the two regimes. In the low w/b ratio regime, the w/b ratio controlled matrix compactness and interfacial quality, significantly affecting compressive and flexural strengths (p = 0.0005 and p = 0.0016, respectively). As the matrix became more susceptible to cracking, the contribution of w/b ratio diminished, whereas steel-fiber bridging became dominant and significantly influenced flexural strength (p = 0.0027). This regime transition demonstrates that the governing mechanism evolves nonlinearly from matrix-controlled strength to fiber-controlled crack resistance. Calcium carbonate whiskers delayed damage initiation through microfilling, crack-tip blunting, and microcrack bridging, but excessive dosages promoted agglomeration and local defects. Steel fibers subsequently restrained macrocrack growth through interfacial bonding, bridging, slip, and pull-out. Together, these actions established a hierarchical toughening mechanism spanning microdefect regulation and macrocrack bridging, transforming abrupt brittle fracture into progressive cracking while sustaining structural integrity. These findings clarify the matrix-dependent nature of multiscale reinforcement and provide a mechanistic basis for regime-specific cementitious composite design through coordinated optimization of matrix quality, microscale crack control, and macroscale bridging.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microcrack evolution and mechanical performance of fiber-reinforced high water-resistant concrete backfill: A quantitative multi-scale studyConstruction and Building Materials · 2026
- Mechanical and Post-Cracking Performance of Recycled and Commercial Steel Fiber-Reinforced ConcreteApplied Sciences · 2026
- Deconstructing Multi-Scale Hybrid Fiber-Reinforced Coarse Aggregate UHPC: From Pore Structure Tailoring to Cross-Scale TougheningMaterials · 2026
- Microstructure-Guided Optimization of Steel Fiber-Reinforced Crumb Rubber Concrete for Sustainable and Lean ConstructionBuildings · 2026
- The Influence of Carbon Fiber Content and Strain Rate on the Mechanical Properties and Microscopic Damage Evolution of Recycled Aggregate Concrete.Materials (Basel, Switzerland) · 2026
- 4D CT–validated mesoscale finite-element modeling and coupled ITZ–fiber damage evolution in micro-steel-fiber-reinforced recycled aggregate concreteConstruction and Building Materials · 2026