Effect of Grain-Boundary Discontinuous Precipitation Evolution on the Transition of Creep-Rupture Failure Modes in Ni-Fe-Based Alloy/Inconel 617 Dissimilar Welded Joints.
Linshu Li, Shengzhi Li, Manjie Fan, Jun Cheng, Wuhua Zhang, Xin Huo, Xia Liu, Kejian Li,
Department of Mechanical Engineering, Tsinghua University, Beijing 100084, China. · Shanghai Turbine Plant, Shanghai Electric Power Generation Equipment Co., Ltd., Shanghai 200240, China.
Key points
From the paper's conclusion- These findings clarify the relationship between grain-boundary DP evolution and creep-rupture failure in Ni-Fe-based alloy/Inconel 617 welded joints, and also provide microstructural guidance for assessing and mitigating creep degradation in dissimilar welded components used in high-temperature A-USC systems.
Abstract
The creep-rupture behavior and microstructural evolution of Ni-Fe-based alloy/Inconel 617 dissimilar welded joints were investigated by creep-rupture testing, interrupted creep testing, and microstructural characterization. Tests were conducted at 630-750 °C under stresses of 130-375 MPa. All joint specimens fractured in the heat-affected zone (HAZ) or base metal (BM) on the Ni-Fe-based alloy side, indicating that the Ni-Fe-based alloy side was the creep-critical region of the joint. Three failure regimes were identified according to the relative rupture lives of the joints and the Ni-Fe-based alloy BM. Fractographic observations revealed predominantly intergranular fracture, with creep cavities and cracks preferentially associated with grain-boundary discontinuous precipitation (DP) regions containing coarsened rod-like γ' precipitates and precipitate-free zones (PFZs). Differences in DP evolution between the HAZ and BM were closely related to creep-damage localization and failure behavior. Interrupted creep tests showed that temperature was the dominant factor affecting DP formation and growth, while applied stress accelerated its evolution. DP developed rapidly during the initial exposure stage and subsequently grew more slowly. These findings clarify the relationship between grain-boundary DP evolution and creep-rupture failure in Ni-Fe-based alloy/Inconel 617 welded joints, and also provide microstructural guidance for assessing and mitigating creep degradation in dissimilar welded components used in high-temperature A-USC systems. Future work should combine longer-term creep testing, phase-resolved microstructural characterization, and predictive modeling to establish quantitative relationships among DP evolution, creep-damage accumulation, and rupture life.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Combined effects of phase transformation–induced PFZ and stress corrosion cracking on the failure of an Inconel 625 boiler tubeEngineering Failure Analysis · 2026
- A Critical Review of Nickel Based Superalloys for Extreme Environments: From Design, Manufacturing to in Service FailureJournal of Manufacturing and Materials Processing · 2026
- Multiscale investigation of gradient growth of intermetallic compounds and joint weakening induced by severe lattice distortion at the interface of Al7075/TC4 friction stir weldsJournal of Materials Research and Technology · 2026
- Achieving serrated grain boundaries within gradient microstructures of nickel-based superalloys for dual-property turbine disks in aeroenginesChinese Journal of Aeronautics · 2025
- Effect of delta processing on microstructure evolution and workability during the high-temperature deformation of Inconel 718Journal of Materials Research and Technology · 2025
- Process control-enabled mitigation of microstructural and plastic heterogeneities in additively manufactured Grade 91 steelJournal of Materials Research and Technology · 2026