Temperature-Dependent Evolution of Coke Structure and Growth Mechanisms of SiC Whiskers Synthesized from Coke and Silicon Powder Under Graphite-Burial Conditions.
Pengcheng Jiang, Huidong Tang, Xin Xiong, Wenting Wang, Xinwei Ou, Kai Chen, Zhiwen Li, Kang Long,
School of Materials Science and Engineering, Hunan Institute of Technology, Hengyang 421002, China.
Key points
From the paper's conclusion- The results reveal that coke exhibits a TG-DSC mass loss of 16.01% and undergoes progressive structural rearrangement and enhanced short-range ordering at 1200-1400 °C while retaining a predominantly turbostratic carbon structure and morphological stability.
Abstract
Silicon carbide (SiC) whiskers are effective reinforcements for carbon-containing refractories; however, their application is restricted by the inherently low reactivity of graphite, which is commonly used as an internal carbon source. In this study, low-cost coke and silicon powder were used as the carbon and silicon sources to synthesize SiC whiskers via a graphite-burial heat treatment process. The structural evolution of coke and the reaction behavior of the coke-Si system at different temperatures were systematically characterized. The results reveal that coke exhibits a TG-DSC mass loss of 16.01% and undergoes progressive structural rearrangement and enhanced short-range ordering at 1200-1400 °C while retaining a predominantly turbostratic carbon structure and morphological stability. At 1100-1200 °C, SiC whiskers form predominantly within pores, and this distribution is consistent with a gas-phase-assisted VS-type growth pathway; the normalized crystalline SiC fractions remain relatively low (~4-11%). A pronounced enhancement of SiC formation occurs at 1300 °C, where the crystalline Si phase becomes undetectable by XRD and abundant SiC whiskers spread from localized pore regions to the matrix surface. The enhanced whisker formation at 1300-1400 °C is attributed to accelerated reaction and mass-transfer processes at elevated temperatures. The synthesized whiskers consist of crystalline β-SiC, and those formed at 1400 °C exhibit high-density stacking faults and pronounced radial coarsening, with representative diameters of approximately 35-80 nm in the TEM images. The structural evolution of coke from a defect-rich state toward a more ordered turbostratic structure occurs concurrently with the temperature-dependent evolution of SiC nucleation and growth and may contribute to the availability of reaction sites and transport pathways, establishing coke as a promising carbon source for the in-situ synthesis of SiC whiskers in refractory applications.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Carbon Precursor-Dependent Si-C Interfacial Reactions and Phase Evolution in Silicon Carbide Synthesis.Langmuir : the ACS journal of surfaces and colloids · 2026
- Regulation of the Silicon–Oxygen Tetrahedral Structure in Fly Ash and Its Effect on the Preparation of β‐SiC WhiskersJournal of the American Ceramic Society · 2026
- Low‐Temperature Densification of SiC Ceramics With Robust Mechanical Properties Using Si–B 4 C AdditiveJournal of the American Ceramic Society · 2026
- Low‐Temperature Solid‐State Sintering of High‐Strength and Electrically Conductive Silicon Carbide With Direct Current Flow and In Situ GraphitizationRare Metals · 2026
- Interfacial adhesion of CVD-SiC coatings on graphite substrates: Role of temperature in microstructure and mechanical propertiesCeramics International · 2025
- A Novel Binder-Assisted Atmospheric Sintering Route for Silicon Carbide (SiC) Production.ACS omega · 2026