Effect of Mechanically Activated Fly Ash, a Superplasticizer, and an Air-Entraining Admixture on the Freeze-Thaw Resistance of Fine-Grained Concrete.
Nazerke Berdikul, Ina Pundienė, Kenzhebek Akmalaiuly, Jolanta Pranckevičienė, Elmira Kurmanbekova, Yerlan Khamza, Aigerim Tolegenova, Assel Kanarbay
Department of Construction and Building Materials, Satbayev University, Satbayev Street 22, Almaty 050013, Kazakhstan. · Laboratory of Concrete Technology, Institute of Building Materials, Vilnius Gediminas Technical University, Linkmenų Str. 28, LT-08217 Vilnius, Lithuania.
Key points
From the paper's conclusion- This study examines how mechanically activated fly ash (TF), a polycarboxylate superplasticizer (PC), and an air-entraining admixture (AE) affect the hydration, microstructure, pore structure, mechanical properties, and freeze-thaw resistance of fine-grained concrete.
Abstract
This study examines how mechanically activated fly ash (TF), a polycarboxylate superplasticizer (PC), and an air-entraining admixture (AE) affect the hydration, microstructure, pore structure, mechanical properties, and freeze-thaw resistance of fine-grained concrete. Mechanical activation increased the specific surface area of the untreated ash (UF) from 3710 to 6450 cm2/g and reduced its mean particle size to 6.06 μm. Replacing 5 wt.% of cement with TF accelerated the nucleation of hydration products and densified the microstructure, as confirmed by exothermic profiling, XRD, and SEM. PC delayed the exothermic peak yet produced the highest heat-release intensity, indicating more efficient wetting and dispersion of reactive surfaces. The TF-PC system reached 39.3 MPa at 28 days, while the ternary TF-PC-AE composition achieved 33.2 MPa with a refined pore-size distribution (mercury intrusion porosimetry). The combined use of PC and AE tripled the pore volume in the 0.01-0.10 μm range and increased it by 28.7% (0.1-1 μm) and 46.21% (1.0-10 μm). The calculated potential freeze-thaw resistance rose from 54.25 to 61.97 and 72.83, confirming the beneficial role of 3-10 μm pores. After 110 accelerated freeze-thaw cycles, the optimized ternary composition lost only 0.55% of its mass.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of Oil Shale Residue on the Frost Resistance of Fly-Ash-Based Autoclaved Aerated Concrete.Materials (Basel, Switzerland) · 2026
- Damage Evolution and Mechanical Deterioration of Concrete Incorporating Waste-Derived Artificial Aggregates Under Freeze–Thaw CyclesSustainability · 2026
- Effects of Tuff Powder on the Macro-Performance and Microstructure of Self-Compacting Concrete under Freeze–Thaw CyclesInternational Journal of Concrete Structures and Materials · 2025
- Freeze-Thaw Damage Evolution of PVA-Fly Ash-Slag Composite Concrete and Low-Dimensional Mapping of Weibull Characteristic Parameters.Materials (Basel, Switzerland) · 2026
- Effect of Fly Ash Mechanical Activation on the Rheology, Hydration, Strength, and Microstructure of Cementitious SystemsInfrastructures · 2026
- Mechanochemically Activated Ternary Modifier Based on Technogenic Mineral Waste for High-Performance Concrete.Materials (Basel, Switzerland) · 2026