Hot Deformation Behavior and Microstructure Evolution of a Novel Near-α Titanium Alloy with Initial Lamellar Microstructure During Hot Compression.
Xiaojuan Jiang, Lili Wu, Tao Sun, Jie Zhou
School of Mechanical Engineering, Chongqing Industry Polytechnic University, Chongqing 401120, China. · College of Mechanical and Vehicle Engineering, Chongqing University, Chongqing 400030, China.
Key points
From the paper's conclusion- The hot deformation behavior and microstructure evolution of a novel near-α Ti65 titanium alloy with an initial lamellar microstructure were investigated by isothermal compression.
Abstract
The hot deformation behavior and microstructure evolution of a novel near-α Ti65 titanium alloy with an initial lamellar microstructure were investigated by isothermal compression. Compression tests were conducted at 950-1010 °C in the α + β phase region and 1050-1110 °C in the β phase region, with strain rates of 0.01-10 s-1 and deformation amounts of 30-75%. The flow behavior, strain-compensated Arrhenius constitutive model, processing map and microstructural evolution were systematically analyzed. The results indicate that the flow stress decreases with increasing temperature and decreasing strain rate, while flow softening is more pronounced in the α + β region than in the β region. The apparent activation energies are 1050.27 kJ/mol for the α + β region and 203.51 kJ/mol for the β region, indicating distinct deformation mechanisms. The established constitutive models exhibit high prediction accuracy, with R and AARE values of 0.98 and 5.97% in the α + β region and 0.99 and 4.29% in the β region, respectively. Processing-map analysis identifies two instability domains at high strain rates: 990-1020 °C/3.5-10 s-1 in the upper α + β region and 1060-1110 °C/1.65-10 s-1 in the β region. Microstructural observations reveal that dynamic spheroidization of lamellar α dominates deformation in the α + β region, whereas dynamic recovery accompanied by limited β dynamic recrystallization occurs in the β region. Increasing deformation amount at 980 °C and 0.01 s-1 promotes α-lamella fragmentation, spheroidization, grain refinement and texture weakening. The maximum pole density decreases to 6.23 mrd at a high deformation amount. By directly correlating strain-dependent processing-map characteristics with quantitative microstructural and crystallographic evolution, this work provides a microstructure-based basis for optimizing the hot-working window of Ti65 alloy with an initial lamellar microstructure.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Investigation on hot deformation behavior of a novel Ti-5Mo-20Nb-10Zr-5Ta-1Fe titanium alloy using constitutive equations, artificial neural network and processing mapsMaterials & Design · 2026
- Hot Deformation Behavior, Dynamic Recrystallization and Phase Transformation Mechanism of Zr-Nb Alloy During Compression Processing.Materials (Basel, Switzerland) · 2026
- High-Temperature Deformation Behavior and Hot Workability of a Ti2AlNb-Based AlloyCrystals · 2026
- Process-dependent microstructural evolution of a hot-deformed damage tolerance titanium alloyJournal of Materials Research and Technology · 2025
- Hot Deformation Behavior of AA3102 Aluminum Alloy: Constitutive Modeling, Microstructural Evolution and Numerical Simulation.Materials (Basel, Switzerland) · 2026
- Constitutive analysis and processing maps revealing the hot deformation mechanisms and workability of N18 zirconium alloyJournal of Materials Research and Technology · 2025