Materials (Basel, Switzerland)

Dual-Function Nitrogen Modification of Phenolic Resin Pyrolytic Carbon: A g-C3N4 Protective Phase and Skeletal Nitrogen Doping for Enhanced Oxidation Resistance.

Pengcheng Jiang, Huidong Tang, Xin Xiong, Wenting Wang, Kang Long, Zhiwen Li, Yongming Kang, Xinwei Ou,

School of Materials Science and Engineering, Hunan Institute of Technology, Hengyang 421002, China.

Key points

From the paper's conclusion
  • These results show that melamine-derived pore regulation and skeletal nitrogen doping jointly retard oxygen transport and suppress oxidation-active defect sites, providing a simple and potentially scalable route for improving the high-temperature oxidation resistance of phenolic resin pyrolytic carbon.

Abstract

Phenolic resin pyrolytic carbon is a key matrix phase in carbon-based refractories and carbon/carbon composites; however, its defect-rich glassy carbon structure exhibits poor oxidation resistance at elevated temperatures. In this work, we report a facile one-step thermal-treatment strategy using melamine as a nitrogen source to prepare nitrogen-modified phenolic resin pyrolytic carbon (NC). The structural evolution and oxidation behavior of samples carbonized at 500-800 °C were systematically investigated by XRD, SEM, TEM, FT-IR, Raman, XPS, BET, and TG-DSC. The results reveal that melamine-derived nitrogen exists in two distinct forms: at 500-700 °C, a carbon nitride-rich phase consistent with graphitic carbon nitride (g-C3N4) forms sheet- and belt-like structures on the carbon surface and partially fills the internal pores; at 800 °C, its long-range crystalline signature disappears, while pyridinic, pyrrolic, and graphitic nitrogen remain in the carbon framework. From 500 to 800 °C, the relative N 1s fraction of pyridinic N decreases from 72.33% to 44.38%, whereas graphitic N increases from 0.47% to 24.09%. Meanwhile, the pore structure evolves from a mesopore-dominated architecture with a limited accessible surface area at 500-600 °C to a micropore-rich structure at 700-800 °C. Relative to unmodified PR-800, NC-800 exhibits an approximately 30 °C higher onset oxidation temperature and an approximately 40 °C higher complete oxidation temperature, together with a lower maximum mass-loss rate and a delayed, broadened exothermic response. These results show that melamine-derived pore regulation and skeletal nitrogen doping jointly retard oxygen transport and suppress oxidation-active defect sites, providing a simple and potentially scalable route for improving the high-temperature oxidation resistance of phenolic resin pyrolytic carbon.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers