Evolution Mechanisms of Microstructure and Performance of Aluminum Alloy Thin-Walled Components Repaired by FrictionStir Spot Welding.
Xiaoming Ye, Jie Zhang, Yuan Liu, Qiu Pang, Yuwei Li
State Key Laboratory of Light Superalloys, Wuhan University of Technology, Wuhan 430070, China. · Department of Mechanical and Electrical Engineering, Wuhan Donghu University, Wuhan 430212, China.
Key points
From the paper's conclusion- Taking the repair of prefabricated hole defects in 2024 aluminum alloy thin-walled componentsby friction stir spot welding (FSSW) as the research object, the evolution lawsof microstructure and mechanical properties of FSSW-repaired joints of thin-walled componentswere clarified through process experiments and numerical simulations.
Abstract
Taking the repair of prefabricated hole defects in 2024 aluminum alloy thin-walled componentsby friction stir spot welding (FSSW) as the research object, the evolution lawsof microstructure and mechanical properties of FSSW-repaired joints of thin-walled componentswere clarified through process experiments and numerical simulations. Thecollaborative effect of the temperature field and material flow field during the FSSW repairprocess and their regulation laws on the microstructure and properties were revealed. Theresults show that as the repair speed increases, the macroscopic surface quality of the FSSWjoint improves. When the repair speed reaches 2000 r/min, a high-quality repaired jointwith a smooth and flat surface and no porosity defects can be obtained. Meanwhile, withinthe repair speed range of 800 to 2000 r/min, the grains undergo dynamic recrystallization(DRX) due to the combined effect of heat and mechanical forces, eventually forming auniform equiaxed grain structure in the weld core area. ABAQUS 2023 simulation verifiesthe temperature distribution during the FSSW repair process. When the repair speed is2000 r/min, the maximum temperature obtained from the simulation is 431.1 ◦C, whichagrees with the measured value from the experiment. The simulation results further revealthat when the repair speed increases from 1200 r/min to 2000 r/min, the material fluiditysignificantly enhances, and the flow velocity on the advancing side is always higher thanthat in other areas. At the rotational speed of 2000 r/min, the plastic material flows continuouslyfrom the periphery and eventually fills the defect area completely. The fracturemode of the FSSW-repaired joint is mainly ductile fracture. With the increase in the repairspeed, the number of dimples at the fracture surface increases significantly. When therotational speed reaches 2000 r/min, the joint achieves the best mechanical properties, andthe FSSW-repaired joint reaches the maximum tensile strength of 169 MPa.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Advancement in fusion welded aluminium alloy joints by friction stir processing technique: a critical reviewDiscover Industrial Chemistry and Materials · 2026
- Microstructure and corrosion resistance of friction stir welded 6061 aluminum alloy joints中国焊接:英文版 · 2026
- Process Parameter Optimization in Refill Friction Stir Spot Welding of 6061-T6 Aluminum Alloy and AZ31B-H24 Magnesium Alloy Dissimilar JointsJournal of Manufacturing and Materials Processing · 2026
- Numerical Investigation of Thermo-Mechanical Response, Tool Contact Stress, and Heat Generation Mechanisms in FSW of AISI 304 Stainless Steel Across Plunge, Dwell, and Travel PhasesCrystals · 2026
- Friction stir welding parameter optimization for dissimilar AA2014 and AA5052 aluminium alloysScientific Reports · 2026
- Effects of the Ratio of Rotation to Welding Speed on the Mechanical Properties of the Friction-Stir Welds of the Dissimilar Aluminum Alloys AA5052-H32 and AA6261-T6Applied Sciences · 2026