Key points
From the paper's conclusion- Unidirectionally macrochanneled tetragonal zirconia polycrystals (TZP) scaffolds, comprising elongated microporous frameworks, were fabricated via vat photopolymerization (VP) using a solution of 75 wt% camphene and 25 wt% 1,6-hexanediol diacrylate (HDDA) as a phase-separable, photopolymerizable vehicle.
Abstract
Unidirectionally macrochanneled tetragonal zirconia polycrystals (TZP) scaffolds, comprising elongated microporous frameworks, were fabricated via vat photopolymerization (VP) using a solution of 75 wt% camphene and 25 wt% 1,6-hexanediol diacrylate (HDDA) as a phase-separable, photopolymerizable vehicle. The camphene/HDDA solution underwent phase separation at 5 °C, accompanied by the recrystallization and dendritic growth of camphene, thereby generating three-dimensionally interconnected camphene crystal networks enclosed by HDDA. Following the photopolymerization of HDDA, the scaffolds were freeze-dried to remove the camphene crystals and subsequently heat-treated for debinding to eliminate organic phases, including photopolymerized HDDA, the dispersant, and the photoinitiator. The effect of sintering temperature on the geometry of the micropores and the densification of the TZP walls was examined. The optimum sintering condition (1500 °C for 3 h) enabled the creation of elongated micropores with a volume fraction of 61.17 ± 0.90 vol%, surrounded by highly densified TZP walls. The fabricated scaffolds exhibited well-defined macrochannels arranged in a hexagonal pattern, separated by microporous frameworks. Their overall porosity was as high as 74.65 ± 0.73 vol%, owing to the high framework microporosity. Despite their high porosity, the scaffolds achieved a compressive strength of 53.10 ± 8.19 MPa and a compressive modulus of 364.38 ± 70.90 MPa.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Digital Light Processing of Reactive Ceramic-Polymer Bone Scaffolds Enables In situ Hydroxyapatite Formation.Acta biomaterialia · 2026
- Sacrificial-Template Fabrication of Orientation-Controlled Porous Titanium Lattices With Bioactive Surfaces.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Poly(ε-caprolactone)-Based Hierarchical Porous Scaffolds Fabricated by a One-Step High Internal Phase Emulsion Templating Method for Bone Tissue Engineering.Polymers · 2026
- Biomechanical and Hydrodynamic Characterization of Gradient-Porosity Triply Periodic Minimal Surfaces Polyether Ether Ketone Scaffolds for Craniofacial Bone Defect Repair.The Journal of craniofacial surgery · 2026
- PDA-Engineered 3D-Printed Polymer-ZrO2 Hybrid Scaffolds Enabling Enhanced Radiopacity, Photothermal Therapy, and Cell Migration Modulation.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Comprehensive Toxicological Evaluation of 3D-Printed Hydroxyapatite (3DPHA) for Bone Grafting ApplicationsInternational Journal of Molecular Sciences · 2026