From the paper's conclusion- This work explores V-alloyed Al0.4Co0.5V0.2FeNi high-entropy alloys that are solution-treated at 1000-1200 °C for five hours and water-quenched.
Abstract
This work explores V-alloyed Al0.4Co0.5V0.2FeNi high-entropy alloys that are solution-treated at 1000-1200 °C for five hours and water-quenched. Solidification of this high-entropy alloy follows the sequence face-centered cubic (FCC) → ordered L12 → body-centered cubic (BCC) → ordered B2. All treated alloys maintain dual FCC-BCC-B2 microstructures, with temperature altering only morphological features. At 1000 and 1100 °C, coherent spinodal decomposition takes place in FCC matrices to form rodlike precipitates with 20.3% lattice misfit; meanwhile, Ostwald ripening lengthens the precipitates from 1.41 to 2.11 μm. Spinodal decomposition is inhibited at 1200 °C, which is accompanied by coarsening and granulation of B2-ordered BCC grains. Slow atomic diffusion prevents recrystallization even above 0.4Tm. Solution heat treatment dissolves the B2 phases to generate supersaturated solutions stronger than the as-cast counterparts. Elevated solution temperatures reduce hardness (243-190 MPa) and tensile strength (919-839 MPa) but boost elongation (26-35%). Fractures display mixed dimple-cleavage features. Overall, a five-hour solution treatment at 1100 °C plus water quenching delivers balanced strength (851 MPa) and ductility (33%), serving as the optimal heat treatment for this alloy.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Al contents on microstructure and mechanical properties of Al CoCrFeNiMo0.3 high-entropy alloysJournal of Materials Research and Technology · 2025
- Improvement of mechanical properties of CoCrFeNiAl0.5 high-entropy alloys treated by double heat-treatment processJournal of Materials Research and Technology · 2026
- Heat-Treatment-Induced Dendritic Structure and Phase Evolution in a Cast AlCrFeMnNiW0.1 High-Entropy AlloyProcesses · 2026
- Effect of Al Content on Microstructure and Mechanical Properties of CoCrFeNiMn High-Entropy AlloyMetals · 2026
- Defect‐Regulated Precipitation Enables Ultrahigh Strength‐Ductility Synergy in a FeCoCrNi‐Based High‐Entropy AlloyRare Metals · 2026
- Multicomponent Si‐Rich σ Phase Induced Deterioration of Ductility and Strain Hardening in a (CoCrNi) 9 Si Medium‐Entropy AlloyAdvanced Engineering Materials · 2026