Investigation into the Mechanical Properties of Swimming-Goggle Gaskets After Prolonged Water Conditioning.
Paulina Maślanka, Laura Kozanecka, Ryszard Korycki, Halina Szafrańska
Department of Mechanical Engineering, Informatics and Chemistry of Polymer Materials, Lodz University of Technology, 90-924 Lodz, Poland. · Lodz University of Technology, 90-924 Lodz, Poland.
Key points
From the paper's conclusion- Overall, the results demonstrate the importance of material selection and geometry optimization and provide a comparative basis for further studies combining environmental conditioning with experimentally calibrated numerical models.
Abstract
This study combines experimental conditioning and numerical simulations to evaluate water-induced degradation of swimming-goggle gaskets and their mechanical response under representative loading conditions. Two gasket geometries were modeled, with the flatter profile serving as a reference and the more anatomically representative variant analyzed using finite-element analysis for neoprene, silicone, and SEBS materials of different Shore A hardness under prescribed periorbital pressure distributions. Commercial gaskets were conditioned by static immersion in chlorinated, distilled, and saline water for 20, 30, and 40 days, followed by measurements of Shore A hardness, breaking force, and elongation at break. The numerical results showed that gasket geometry substantially influences the predicted deformation patterns relevant to facial conformability, despite similar overall deformation magnitudes. Prolonged water exposure caused considerable material degradation. The breaking force decreases by approximately 48% after 20 days and by about 50% after 40 days of conditioning, irrespective of the environment. Elongation at break changed by approximately 3-4% in chlorinated and distilled water, whereas saline water caused reductions of approximately 11% after 20 days and 36% after 40 days. Additionally, the hardness of the material drops by about 10-13% after 20 days and subsequently remains almost constant. In the adopted cyclic loading-recovery simulation, silicone exhibited substantially lower residual deformation than SEBS. Overall, the results demonstrate the importance of material selection and geometry optimization and provide a comparative basis for further studies combining environmental conditioning with experimentally calibrated numerical models.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effects of Natural Ageing on the Dimensional, Mechanical, and Thermal Properties of Diving Neoprene.Polymers · 2026
- Systematic Benchmarking of a Noise‐Tolerant Conductive Hydrogel Electrode for Epidermal BioelectronicsAdvanced Science · 2025
- Hydrogen Compatibility of Commercial Silicone Elastomer Seals: Multiscale Mechanical and Surface Characterization Following High-Pressure Hydrogen Exposure.Polymers · 2026
- Mechanical and Gravimetric Response of Surgical Suture Biomaterials to Commercial Mouthrinses During Static In Vitro Exposure.Bioengineering (Basel, Switzerland) · 2026
- Overcoming challenges in the chemical analyses of wound dressings: a practical approach based on solvent compatibility.Regulatory toxicology and pharmacology : RTP · 2026
- Tribological Performance of Glass/Kevlar Hybrid Epoxy Composites: Effects of Pressurized Water-Immersion Aging Under Reciprocating Sliding WearPolymers · 2025