Effect of Welding Heat Input on Microstructure and Properties of CGHAZ in Deep-Sea Oil and Gas Transportation Pipeline Steel.
Lili Ran, Shilin Liu, Ba Li, Yanan Li, Rui Hong, Bing Wang, Qingyou Liu, Shujun Jia
Department of Structural Steels, Central Iron and Steel Research Institute Co., Ltd., Beijing 100081, China. · Construction Project Management Branch of China Oil and Gas Pipeline Network Group Co., Ltd., Langfang 065001, China.
Key points
From the paper's conclusion- The results show that as the Cr content increases, the range of valid welding heat input for maintaining satisfactory CGHAZ impact toughness gradually narrows with increasing Cr mass fraction of the steel.
Abstract
Gleeble-3800 thermal simulation testing machine was adopted to investigate the evolution laws of microstructure and properties in the coarse-grained heat-affected zone (CGHAZ) of pipeline steels with different Cr mass fractions (0.2, 0.5, 0.8 wt.%) under welding heat inputs ranging from 8 kJ/cm to 20 kJ/cm. Combined with optical microscopy, scanning electron microscopy and electron backscatter diffraction, the coupled influencing mechanism of heat input and Cr content on the properties of CGHAZ was systematically analyzed. The results show that as the Cr content increases, the range of valid welding heat input for maintaining satisfactory CGHAZ impact toughness gradually narrows with increasing Cr mass fraction of the steel. Specifically, the 0.2Cr experimental steel maintains high toughness under a thermal input ranging from 8 to 20 kJ/cm, the 0.5Cr experimental steel exhibits relatively high toughness in the range 8 to 13 kJ/cm, while the 0.8Cr experimental steel shows high toughness only at 15 kJ/cm. The coupled effect of weld heat input and Cr content on CGHAZ properties originates from a combination of microstructural composition types, phase fractions, substructures, and grain sizes. Increasing the heat input and Cr content leads to a reduction in the bainite ferrite with superior toughness and an increase in the large-sized granular bainite with inferior toughness. Meanwhile, the effective grain size of the overall microstructure first decreases and then rises. Grain coarsening and an increased fraction of Martensitic/Austenitic (M/A) constituent are the key factors responsible for the deterioration of CGHAZ toughness in deep-sea oil and gas transportation pipeline steel.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of heat input on microstructure and impact toughness of X80 FCAW-S weld jointJournal of Materials Research and Technology · 2026
- Tailored heat treatments to characterise the fracture resistance of critical weld regions in hydrogen transmission pipelinesInternational Journal of Hydrogen Energy · 2025
- Structural Integrity of Welded Pipe Joints Made of Creep–Resistant Steel P91 with Multiple Defects: Experimental Characterization and Engineering Critical AssessmentMetals · 2026
- Analysis of the weakest regions and microstructural features influencing impact toughness in Q690 high-strength steel welded jointsJournal of Materials Research and Technology · 2026
- Effect of Heat Input on the Microstructure and Mechanical Properties of AISI 316 stainless steel TIG Welded tube Jointsمجلة غريان للتقنية · 2026
- Optimizing impact toughness in Q1100E steel welds via laser-arc hybrid welding energy ratio controlJournal of Materials Research and Technology · 2026