Optimization of Mix Proportions for Type IV Cement-Based Grouting Materials Using Orthogonal Experimental Design.
Binghao Wang, Yong Xu, Yingda Zhang, Ziqiang Lyu, Zhen Wang, Meiling Gu
Chengdu Urban Construction Investment Management Group Co., Ltd., Chengdu 610037, China. · School of Architecture and Civil Engineering, Xihua University, Chengdu 610039, China.
Key points
From the paper's conclusion- Based on the comprehensive evaluation, the optimal mix proportion was determined as A3B2C4D2, corresponding to a water-to-binder ratio of 0.31, a fly ash content of 15%, a total binder content of 690 kg/m3, and a silica fume content of 8.5%.
Abstract
This study systematically investigates the effects of water-to-binder ratio, total binder content, silica fume content, and fly ash content on the fluidity and compressive strength of Type IV cement-based grouting materials. An L16(44) orthogonal experimental design was adopted to evaluate the influence of these four factors on initial and 30 min slump flow, as well as 1-day, 3-day, and 28-day compressive strength. The range analysis results indicate that silica fume content exerts the most significant effect on initial slump flow, while the water-to-binder ratio predominantly governs the 30 min slump flow and early-age compressive strength, such as at 1 day and 3 days. The total binder content is identified as the key factor influencing the 28-day compressive strength. Furthermore, supplementary tests on the combined incorporation of fly ash and silica fume reveal that silica fume enhances early-age strength but reduces fluidity, whereas fly ash improves fluidity but promotes later-age strength development, with an optimal substitution range for both admixtures. Microstructural analyses including XRD and SEM and hydration heat tests further elucidate the underlying mechanisms, demonstrating that the effects of the two admixtures optimize the hydration process and microstructure densification. Based on the comprehensive evaluation, the optimal mix proportion was determined as A3B2C4D2, corresponding to a water-to-binder ratio of 0.31, a fly ash content of 15%, a total binder content of 690 kg/m3, and a silica fume content of 8.5%. This optimized formulation achieves a balanced performance in both workability and strength development.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Mix-Proportion Evaluation and Microstructural Characteristics of NaOH-Na2SO4 Composite-Activated Fly Ash-Based Grouting Materials.Materials (Basel, Switzerland) · 2026
- Optimization of Multi-Component Cement Mortar Using a Taguchi Orthogonal Array Design.Materials (Basel, Switzerland) · 2026
- Optimization of the mix ratio and performance mechanism research of composite cement-based slope filling and protection materials.Science progress · 2026
- Sustainable high-performance injection geopolymers, role of GGBFS and water-to-binder ratio in strength, microstructure, and predictive modelingScientific Reports · 2025
- Material-Medium Performance Transferability of Two Modified Cementitious Grout Systems.Materials (Basel, Switzerland) · 2026
- Synergistic optimization of nanosilica sol-calcium aluminate cement composite grout by silica micropowder: Effects on microstructure and sealing performanceCase Studies in Construction Materials · 2026