From the paper's conclusion- The corrosion behavior of symmetric (S-joint) and asymmetric (A-joint) double-sided friction stir-welded (DS-FSW) 7A65 aluminum alloy thick plates was investigated in 3.5 wt% NaCl solution.
Abstract
The corrosion behavior of symmetric (S-joint) and asymmetric (A-joint) double-sided friction stir-welded (DS-FSW) 7A65 aluminum alloy thick plates was investigated in 3.5 wt% NaCl solution. The S-joint, produced using the same large tool (Φ30 mm) for both passes, imposes two high-heat thermal cycles that result in insufficiently fragmented intermetallic particles (IMPs), coarse grains, and severely overaged heat-affected zones (HAZs). In contrast, the A-joint, employing a smaller tool (Φ24 mm) for the second pass, reduces the total heat input and achieves a refined microstructure with fine (2-3 µm), rounded IMPs in the second-pass weld nugget (WNZ-S) and less degraded HAZs. Electrochemical measurements reveal that the HAZ-Overlap (HAZ-O) is the most anodic zone in both joints. The S-joint shows a larger potential spread (up to ~120 mV) and higher corrosion current density than the A-joint. The hierarchical galvanic coupling, where macro-galvanic corrosion between the anodic HAZ-O and cathodic WNZs drives severe localized attack, while micro-galvanic corrosion around coarse IMPs initiates trenching, is elucidated. The A-joint mitigates this damage due to its reduced galvanic driving force (smaller potential spread of ~74 mV) and improved microstructural homogeneity. The enhanced corrosion resistance of the A-joint is attributed to grain refinement, effective IMP fragmentation, and a less degraded HAZ microstructure.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructure and corrosion resistance of friction stir welded 6061 aluminum alloy joints中国焊接:英文版 · 2026
- Mechanical and electrochemical analysis of AA5083-AA7075 dissimilar alloy joints fabricated by friction stir weldingDiscover Materials · 2026
- Microstructural characteristics, mechanical properties, and corrosion behavior of FSW dissimilar joints between Al-Zn-Mg-(Sc-Zr) and Al-Mg-Si alloysJournal of Materials Research and Technology · 2026
- Quasi-Static and Fatigue Behavior of Dissimilar Friction Stir Welded Aluminum Joints Subjected to Acetic Acid Salt Spray ExposureMaterials · 2026
- Corrosion behaviour of friction stir welded dissimilar magnesium alloys ZE41 and AZ31Materialwissenschaft und Werkstofftechnik · 2026
- Friction stir welding of dissimilar metals: Investigating the role of interlayers in aluminium-steel butt joint performanceMaterials Today Communications · 2025