Materials (Basel, Switzerland)

A Comparative Study on Microstructure and Mechanical Properties of Ti-6Al-4V Fabricated by Laser/Electron Beam Powder Bed Fusion.

Yaojia Ren, Jingru Wang, Jiajun Xu, Yingkang Wei, Jilei Zhu, Qingge Wang, Jianyong Wang, Shifeng Liu,

School of Metallurgical Engineering, Xi'an University of Architecture and Technology, Xi'an 710055, China. · State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China.

Key points

From the paper's conclusion
  • To address the strength-ductility trade-off in titanium alloys, a comparative study was conducted on Ti-6Al-4V (TC4) alloys fabricated by laser powder bed fusion (L-PBF) and electron beam powder bed fusion (EB-PBF).

Abstract

To address the strength-ductility trade-off in titanium alloys, a comparative study was conducted on Ti-6Al-4V (TC4) alloys fabricated by laser powder bed fusion (L-PBF) and electron beam powder bed fusion (EB-PBF). The L-PBF specimen primarily consisted of acicular α' martensite with high residual stress. In contrast, the EB-PBF specimens, owing to a substrate preheating temperature of 740 °C and a reduced cooling rate (103~105 K/s), exhibited a stable and coarse α + β lamellar structure. Combined with the high oxygen content (0.24 wt.%) that provided solid-solution strengthening, this morphology enabled simultaneous attainment of a yield strength of 1120 ± 12 MPa and an elongation at fracture of 11.1 ± 1.3%. Notably, deformation-induced HCP→FCC phase transformation occurred in EB-PBF alloys, generating a dual-phase HCP/FCC structure that effectively accommodated plastic strain. These results highlight the superior potential of EB-PBF over L-PBF for fabricating titanium alloys with an exceptional strength-ductility synergy.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers