From the paper's conclusion- The obtained results demonstrate that porous poly(DMN-co-TRIM) microspheres constitute promising thermally stable materials with tunable porous structure and potential applications in chromatographic separation techniques.
Abstract
Porous microspheres based on 1,4-(dimethacryloyloxymethyl)naphthalene (DMN) and trimethylolpropane trimethacrylate (TRIM) were obtained by suspension-emulsion polymerization in the presence of toluene as a porogenic diluent. The obtained copolymers were subsequently modified using tetrachloromethane in the presence of anhydrous AlCl3 via a Friedel-Crafts-type reaction. The influence of monomer composition and post-polymerization modification on the porous structure parameters and thermal stability of the materials was investigated. The synthesized copolymers exhibited well-developed porous structures with surface areas ranging from 368 to 494 m2/g. Increasing the TRIM content resulted in higher crosslinking density, earlier phase separation during polymerization, and formation of a finer porous architecture characterized by increased surface area and lower pore diameters. Chemical modification caused moderate and composition-dependent changes in the porous structure while preserving the mesoporous character of the materials. The highly crosslinked copolymers demonstrated the greatest structural stability during modification. Thermogravimetric analysis performed in helium revealed high thermal resistance of both parent and modified copolymers. The degradation process proceeded in two main stages characteristic of highly crosslinked methacrylate networks. Increasing TRIM content improved resistance toward advanced thermal decomposition, increasing the T50% values up to 415 °C. Post-polymerization modification slightly decreased the temperature of the second degradation stage, probably due to the introduction of thermally less stable chlorinated fragments, while simultaneously increasing char residue formation. The synthesized materials were also evaluated as stationary phases for gas chromatography. Owing to their high thermal stability and the presence of polar ester functionalities, the copolymers enabled efficient separation of aliphatic alcohols at elevated temperatures. The obtained results demonstrate that porous poly(DMN-co-TRIM) microspheres constitute promising thermally stable materials with tunable porous structure and potential applications in chromatographic separation techniques.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Hansen Solubility Parameter Analysis of Pore Structure Regulation in Porous Polystyrene Microspheres with Temperature-Dependent Adsorption after NIPAM ModificationLangmuir · 2026
- Depolymerization of Commercial Polymethacrylates Triggered by Hydroperoxides.Journal of the American Chemical Society · 2026
- Performance Evaluation on Profile Control and Flooding of QPD Thermosensitive Gel in High-Temperature and High-Salinity Reservoir of Block X.Molecules (Basel, Switzerland) · 2026
- Synergistic Rigid-Flexible Cross-Linking via Thiol-Modified POSS for High-Performance Thermally Expandable Microspheres with Extended Foaming Range and Enhanced Expansion.Langmuir : the ACS journal of surfaces and colloids · 2026
- 3D‐Printable Nanoporous Thermosets via Disulfide‐Based Polymerization‐Induced Microphase SeparationAngewandte Chemie International Edition · 2026
- Polymer-Dependent Morphology Development of Biodegradable Porous Microspheres with Amphiphilic PEG-PDLLA Incorporation.Polymers · 2026