Influence of Base Plate Preheating on Laser Powder Bed Fusion–Processed EN AW-7075 Aluminium Alloy
Nejc Velikajne, Jožef Medved, Črtomir Donik, Irena Paulin
University of Ljubljana · Institute of Metals and Technology
Key points
From the paper's conclusion- The results demonstrate that base plate preheating alone is insufficient to suppress hot cracking in EN AW 7075 and may promote alternative crack-growth mechanisms at elevated temperatures, highlighting the need for alternative alloy or process design strategies.
Abstract
The influence of base plate temperature (25, 100, 200, and 400 °C) on the laser powder bed fusion processing of EN AW 7075 was systematically investigated using microstructural characterisation (LM, SEM, EBSD, GROD), chemical analysis, hardness testing, and thermal simulations across a broad range of process parameters. Moderate preheating at 100 °C and 200 °C showed no significant reduction in crack density or changes in grain morphology compared to processing without preheating. At the highest studied temperature-400 °C-a transition to columnar crack networks was observed, accompanied by modified grain orientation, pronounced stress relaxation, and reduced hardness. Independent of preheating temperature, consistent evaporation of Zn (~1 wt.%) and Mg (~0.3 wt.%) occurred during processing. Thermal simulations qualitatively supported the experimental observations, indicating increased thermal retention and displacement with increasing preheating temperature. The results demonstrate that base plate preheating alone is insufficient to suppress hot cracking in EN AW 7075 and may promote alternative crack-growth mechanisms at elevated temperatures, highlighting the need for alternative alloy or process design strategies.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- A data-based approach for predicting hardness in friction stir additive manufacturing of EN AW-7075-T6Progress in Additive Manufacturing · 2026
- Mechanical behavior of Al6061 produced by laser powder bed fusion: Effects of heat treatments and strain ratesMaterials Science and Engineering A · 2025
- Toward post-process-free fatigue performance: In-situ heating and heat treatment of additively manufactured IN718Journal of Alloys and Compounds · 2025
- Optimization of laser powder bed fusion process to enhance mechanical properties of as-built Ti–6Al–4V samplesJournal of Materials Research and Technology · 2025
- Multi-parameter optimization of laser powder bed fusion process for pure Zn-based biodegradable implantsAdditive Manufacturing Frontiers · 2026
- Post-process heat treatment design for tunable strength and toughness in L-PBF 2507 super duplex stainless steelMaterialia · 2026