Lubricants

Study on the Effects of Mo on the Micro-Structure and Wear Resistance of CuCrZr Plasma Cladding Coatings

Genrong Cao, Yang Wang, Chunyan Liang, Zhiming Qiao, Xichao Yuan, Ran Zhao

Key points

From the paper's conclusion
  • The results show that the addition of 0.3 wt.% Mo produces the finest grains, the highest Rockwell hardness of 87.9 HRB (8.4% higher than the Mo-free coating), the lowest average friction coefficient of 0.280 (a 10.8% reduction), and the lowest wear mass loss of 5.70 mg (38.7% lower than the bare substrate).

Abstract

Under extreme current densities, the sliding contact between the armature and the CuCrZr rail of an electromagnetic railgun induces transition ablation, planing, and groove erosion, which severely shorten the service life of the launch track. CuCrZr–Mo composite coatings containing 0, 0.15, 0.3, and 0.45 wt.% Mo were deposited on a CuCrZr substrate by plasma cladding to enhance the tribological performance of the rail. The microstructure, phase composition, hardness, electrical resistivity, friction and wear behaviour, and coating/substrate bond strength were systematically characterised. The results show that the addition of 0.3 wt.% Mo produces the finest grains, the highest Rockwell hardness of 87.9 HRB (8.4% higher than the Mo-free coating), the lowest average friction coefficient of 0.280 (a 10.8% reduction), and the lowest wear mass loss of 5.70 mg (38.7% lower than the bare substrate). However, the resistivity rose from 2.0 × 10−6 Ω·cm at 0.15 wt.% Mo to 3.0 × 10−6 Ω·cm at 0.3–0.45 wt.% Mo, and the bond strength decreased monotonically with increasing Mo, indicating a trade-off between wear life and electrical/mechanical integrity. The findings offer a practical guideline for selecting Mo additions to extend the operational life of electromagnetic railgun tracks.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers