Comparative Evaluation of HVOF-Sprayed WC-12Co Coatings: Load and Contact Effects on Cross-Sectional Scratch Resistance and Dry Sliding Wear
Bauyrzhan Rakhadilov, Nurtoleu Magazov, Aidar Kengesbekov, Małgorzata Rutkowska-Gorczyca, Dauir Kakimzhanov, Elvira Akhmetova
Key points
From the paper's conclusion- The different rankings obtained from hardness, scratch damage, and wear measurements show that the coating response depends on the deformation scale and contact conditions.
Abstract
WC-12Co coatings deposited by liquid-fuel high-velocity oxy-fuel (HVOF) spraying at kerosene pump frequencies of 33, 35, and 37 Hz were evaluated by cross-sectional scratch testing at 5–25 N and dry sliding at a constant load of 10 N. F35 exhibited the highest mean Martens hardness (9.42 GPa), whereas F33 had the smallest mean projected scratch-damage area at 5–15 N. On ground surfaces, F35 showed the lowest specific wear rates in reciprocating and ball-on-disc tests: 3.61 × 10−6 and 5.69 × 10−5 mm3 N−1 m−1, respectively. For the as-sprayed surface under reciprocating sliding, the lowest value was obtained for F37. Wear results represent one test per coating in each configuration. SEM/EDS observations were consistent with local material removal, transfer from the steel counterbody, and the formation of oxygen-enriched regions. The different rankings obtained from hardness, scratch damage, and wear measurements show that the coating response depends on the deformation scale and contact conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Kerosene Feed Rate on In-Flight Particle Behavior and Resulting Phase Composition, Microstructure and Mechanical Properties of HVOF-Sprayed WC–12Co CoatingsJournal of Manufacturing and Materials Processing · 2026
- Parametric investigation of air jet erosion behavior of CrB₂ - and TiC-reinforced high velocity oxy-fuel (HVOF) sprayed WC–12Co coatingsIronmaking & Steelmaking Processes Products and Applications · 2026
- Effect of Deposition Defects on the Wear and Corrosion Resistance Behavior of HVOF-Sprayed 304 Stainless Steel CoatingsCoatings · 2026
- Influence of Gas Flow Rates in Kerosene-Fueled HVOF Spraying on the Microstructure, Phase Composition, and Corrosion Behavior of Cr3C2-NiCr CoatingsCoatings · 2026
- Effect of WC-NiCrBSi/NiCuBSi based coatings on wear performance of austenitic stainless steelMaterials Testing · 2026
- Comparative study on the morphology and tribological behaviour of Co/WS₂ , Co/WC, and hybrid Co/WC–WS₂ composite coatingsTransactions of the IMF · 2026