Osteoblast-like Cell Response to Titania-Ca-Modified Siloxane Biohybrids.
Ricardo Iván Gutiérrez-Ventura, Hugo Iván Arrieta-Oliva, Daniela Anahí Sánchez-Téllez, Manuel Alejandro Mosso-Pani, Blanca Estela García-Pérez, Lucía Téllez-Jurado
Departamento de Ingeniería en Metalurgia y Materiales, Escuela Superior de Ingeniería Química e Industrias Extractivas, Instituto Politécnico Nacional. Av. Instituto Politécnico Nacional S/N, Lindavista, Mexico City 07738, Mexico. · Departamento de Microbiología, Escuela Nacional de Ciencias Biológicas, Instituto Politécnico Nacional. Prolongación de Carpio y Plan de Ayala S/N, Casco de Santo Tomás, Mexico City 11340, Mexico.
Key points
From the paper's conclusion- The findings suggest that titania enhances the biocompatibility of siloxane materials and shows significant potential for bone tissue regeneration without added growth factors.
Abstract
This study examined the response of osteoblast-like cells to siloxane-based biohybrid materials obtained via the sol-gel process and modified with titania or with titania and calcium. The biohybrids' ability to form apatite and their degradation process were assessed in vitro via immersion in PBS and SBF. Characterization was performed using XRD, FT-IR, and SEM. The Siloxane-Ti biohybrid exhibited rutile crystalline phase formation, high stability, and resistance to hydrolytic degradation, but did not induce apatite growth. In contrast, the Ca-containing biohybrid showed a vitreous structure with significant surface morphology changes and increased degradability. The Ca-modification enhanced the precipitation of apatite layers, which was attributed to the presence of Ti-OH and Si-OH groups. Immersion of the Siloxane-Ti-Ca biohybrids in PBS produced a flake-like apatite-like mineral structure from the first day of immersion, while immersion in SBF led to a cauliflower-like apatite structure after 28 days. Osteoblast response was evaluated through cell adhesion, proliferation, and differentiation on the hybrid materials. The Siloxane-Ti hybrid promoted osteoblast adhesion and proliferation, whereas the Siloxane-Ti-Ca reduced cell viability and osteonectin expression at 21 days. The Siloxane-Ti hybrid also increased osteonectin expression at early stages, with osteopontin and osteocalcin expression emerging at later stages, indicating progression from early to mature stages stimulated by the hybrid material. The findings suggest that titania enhances the biocompatibility of siloxane materials and shows significant potential for bone tissue regeneration without added growth factors.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Hydrocalumite‐Like Material Induces Early Osteogenic Priming and ECM Remodeling Without Effective Mineralization in PreosteoblastsJournal of Biomedical Materials Research Part A · 2026
- In Vitro Evaluation of Novel Calcium Silicate‐Based and Resin‐Modified Calcium Silicate Materials: Cytocompatibility and Mineralization Potential on Human Dental Pulp Stem Cells for Pulp RepairMicroscopy Research and Technique · 2026
- Multifunctional Rare-Earth-Ion-Doped Si-HAp Platforms Modulate Human BMSC Lineage-Associated Molecular Responses Without Enhancing Terminal DifferentiationbioRxiv · 2026
- Early Osteogenic Transcriptional Response of Pre-Osteoblastic Cells on Biomorphic Mg2+-Doped Biphasic Calcium Phosphate Scaffolds.Cells · 2026
- Evaluation of the Physicochemical and Biological Properties of Calcium-Silicate-Based Root-End Filling MaterialsJournal of Functional Biomaterials · 2026
- Functionalized BLGFs/ODEX hydrogel scaffold incorporating Oreochromis lidole skin collagen for bone tissue regenerationRegenesis repair rehabilitation. · 2026