Role of Porosity in Mechanical Performance of 6061 Al Alloy Fabricated via Wire Arc Additive Manufacturing
Hang Zhang, Yong Song, Rongguang Li, Zhihao Zhao, Yuehong Zhang, Peijun Yang, Shanshan Li, Zehua Li,
Key points
From the paper's conclusion- These results reveal a competing mechanism in as-deposited 6061 alloy, in which the ductility benefit of porosity suppression fully over-rides the classical detrimental effects of grain and secondary-phase coarsening, indicating that pore mitigation, rather than grain refinement, should be assigned the highest priority in the process optimization of WAAM Al alloys.
Abstract
In this work, two distinct microstructural configurations were designed for wire arc additive manufacturing (WAAM) of 6061 Al alloy to elucidate the role of porosity in governing mechanical performance. The two samples exhibited contrasting porosity levels—an area fraction of 1.3% with an average pore size of 26.0 μm for one sample versus 3.4% and 29.8 μm for the other—while the low-porosity sample possessed coarser grains, higher dislocation density, and more densely distributed grain-boundary secondary phases, conventionally regarded as detrimental. Despite these unfavorable characteristics, the low-porosity sample had not only a higher ultimate tensile strength (183–190 MPa vs. 170–177 MPa) but also a substantially larger elongation (18.6–19.2% vs. 6.2–10.7%) and a drastically lower tensile anisotropy (3.2% vs. 42.1%). The elevated porosity of the high-porosity configuration introduced abundant stress concentration sites and provided preferential pathways for crack initiation and propagation, triggering premature fracture and severely curtailing the uniform plastic deformation stage. In contrast, the reduced porosity effectively suppressed crack nucleation, prolonged the uniform deformation stage, and fully compensated for the adverse effects of grain coarsening and secondary-phase coarsening. These results reveal a competing mechanism in as-deposited 6061 alloy, in which the ductility benefit of porosity suppression fully over-rides the classical detrimental effects of grain and secondary-phase coarsening, indicating that pore mitigation, rather than grain refinement, should be assigned the highest priority in the process optimization of WAAM Al alloys.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- The effect of standard heat treatments and process conditions on the fatigue performance of wire arc additively manufactured Ti-6Al-4VMaterials Science and Engineering A · 2026
- Ultrasonic-assisted wire arc additive manufacturing significantly improves impact toughness of 5183 aluminum alloyJournal of Materials Research and Technology · 2026
- Mechanical behavior of Al6061 produced by laser powder bed fusion: Effects of heat treatments and strain ratesMaterials Science and Engineering A · 2025
- In Situ Formation of L1 2 ‐Al 3 Ti Precipitates Enabling High Strength and Toughness in Oscillating Laser‐Welded Aluminum AlloyRare Metals · 2026
- Multi scale performance breakthrough of Sc/Zr/Mn microalloying controlled wire arc additive manufacturing of high-strength light alloysVirtual and Physical Prototyping · 2025
- Ultrasonic-Based Quantification and Process Parameter Optimization of Anisotropy and Heterogeneity in WAAM 2319 Aluminum AlloyMaterials · 2026