Defect-Related Low-Temperature Luminescence of Undoped Biogenic Carbonate-Containing Hydroxyapatite Under VUV Synchrotron Excitation.
Zhakyp T Karipbayev, Dulat H Daurenbekov, Keleshek B Zhangylyssov, Rakhima K Daurenbekova, Guldari B Bairbayeva, Aizat Bakytkyzy, Askhat Kakimov, Anatoli I Popov
Department of Technical Physics, Institute of Physics and Technology, L.N. Gumilyov Eurasian National University, Kazhymukan Str. 13, Astana 010008, Kazakhstan. · Department of Thermal Power Engineering, Faculty Transport and Energy, L.N. Gumilyov Eurasian National University, Kazhymukan Str. 13, Astana 010008, Kazakhstan.
Key points
From the paper's conclusion- Defect-related self-activated luminescence of unintentionally undoped biogenic carbonate-containing hydroxyapatite (HAp) was studied at 12 K under tunable vacuum-ultraviolet excitation at the P66 beamline of PETRA III.
Abstract
Defect-related self-activated luminescence of unintentionally undoped biogenic carbonate-containing hydroxyapatite (HAp) was studied at 12 K under tunable vacuum-ultraviolet excitation at the P66 beamline of PETRA III. X-ray diffraction confirmed the hexagonal P63/m apatite framework and an apparent coherent-domain size of approximately 57.7 nm. Raman spectroscopy verified the phosphate framework, B-type carbonate near 1072 cm-1, and a perturbed structural-OH environment, while not identifying defect charge states. Four empirical emission families were resolved at 2.530, 2.995, 3.305, and 3.630 eV. PLE monitored at 504, 426, 375, and 346 nm covers D1-D4 and reveals common excitation regions near 5.3-5.5, 6.1, and 7.06-7.10 eV, together with D2-selective and D4-selective features near 6.50 and 9.83 eV. The D3-centred 375 nm profile is dominated by the 7.10 eV component. Hybrid-functional and G0W0 calculations place the ideal-HAp edge near 7.1-7.5 eV; therefore, the common near-7.1 eV PLE feature is treated as the best-supported host-related near-edge/excitonic marker, whereas lower-energy features are assigned cautiously to localized sub-gap absorption. Because PLE is not a direct absorption measurement, the pathway scheme is presented as a conceptual hypothesis rather than a uniquely resolved kinetic model.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Low-cost and sustainable hydroxyapatite synthesis using technical-grade phosphoric acid for environmental applications: Structural and morphological insightsOpen Ceramics · 2025
- Effect of Eu 3+ Addition on the Structural, Morphological, and Luminescent Properties of Hydroxyapatite Nanostructures Synthesized by Microwave‐Assisted Hydrothermal MethodCrystal Research and Technology · 2026
- First-Principles Modelling of Ion-Substituted Hydroxyapatite: Defect Chemistry, Site Preferences, and Structure-Property Relationships-A Critical Review.Biomimetics (Basel, Switzerland) · 2026
- Multifunctional Rare-Earth-Ion-Doped Si-HAp Platforms Modulate Human BMSC Lineage-Associated Molecular Responses Without Enhancing Terminal DifferentiationbioRxiv · 2026
- Physicochemical Comparison of Hydroxyapatite Extracted from Adult and Young Duroc-Jersey Porcine Bones: Influence of Predominant Ionic Composition on Enhanced Potential Applications.ACS omega · 2026
- Influence of single and co-doped lanthanides on the thermoluminescence response of hydroxyapatite prepared by the hydrothermal method.Radiation and environmental biophysics · 2026