Concentration-Dependent Human Serum Albumin Layers on Ti-6Al-4V Modulate Mammalian Cells and S. aureus Responses.
Mandana Azari, Zhongqian Xi, Christof Neumann, Julius Trautmann, Andrey Turchanin, Oliwia Makarewicz, Klaus D Jandt, Britt Wildemann
Experimental Trauma Surgery, Department for Trauma-, Hand- and Reconstructive Surgery, Jena University Hospital, Friedrich Schiller University Jena, Am Klinikum 1, 07747 Jena, Germany. · Jena School for Microbial Communication (JSMC), Friedrich Schiller University Jena, Neugasse 23, 07743 Jena, Germany.
Key points
From the paper's conclusion- Overall, these findings demonstrate a concentration-dependent response to HSA-modified Ti-6Al-4V, with favourable short-term cytocompatibility at higher coating concentrations and reduced S. aureus adhesion at the highest concentration tested.
Abstract
Orthopaedic Ti-6Al-4V implants face two persistent risks: early infection and limited osseointegration. Human serum albumin (HSA) coatings may influence interactions between titanium interfaces in both mammalian and bacterial cells, but these effects may depend on the concentration used during coating preparation. In this study, Ti-6Al-4V discs were PEI-functionalized and coated with HSA solutions ranging from 200 to 500 µg·mL-1. Surface properties were assessed by AFM, contact-angle goniometry, and XPS, while apparent surface-associated HSA and short-term coating retention were estimated using a BCA depletion approach. The apparent surface-associated HSA, estimated from solution depletion, increased with increasing coating concentration, and all coated samples remained ultrasmooth (Ra < 1 nm), providing a comparable physical baseline. In FBS-free DMEM, at least 70% of the initially estimated HSA remained after 3 days. SaOS-2 metabolic activity was reduced at coating concentrations of 200-300 µg·mL-1, whereas at concentrations of 400-500 µg·mL-1 the values did not differ from polished Ti-6Al-4V after 72 h. LDH release remained unchanged across groups. No significant changes were observed in the expression of osteogenic markers and miRNAs analysed among the HSA-coated samples. Macrophage-like cell (THP-1) attachment was reduced on HSA-coated surfaces, while inflammatory gene expression remained largely unchanged. S. aureus adhesion was quantified by CFU counting after 3 h and 24 h, and SEM analysis after 3 h. When culturing S. aureus on 500 µg·mL-1 coated discs, an approximately 1-log10 reduction in recoverable S. aureus CFU vs polished Ti-6Al-4V was observed. Overall, these findings demonstrate a concentration-dependent response to HSA-modified Ti-6Al-4V, with favourable short-term cytocompatibility at higher coating concentrations and reduced S. aureus adhesion at the highest concentration tested.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- B-168 Purified Recombinant Human Albumin Produced in Thermothelomyces heterothallica (C1) Demonstrates Effective Blocking and Comparable Surface Binding to Other Recombinant and Native AlbuminsClinical Chemistry · 2026
- Human Serum Albumin Preserves Delivered Dose and Suspension Stability During Simulated Clinical Infusion of Mesenchymal Stromal Cells.European journal of pharmaceutical sciences : official journal of the European Federation for Pharmaceutical Sciences · 2026
- Study on the Influence of Hydroxyapatite on Human Cell Viability and Adhesion in Chemical Antibacterial Silver CoatingsDentistry Journal · 2026
- Osteoimmunomodulation by functional protective coatings: tuning innate and adaptive immunity for titanium implant osseointegrationReports of Morphology · 2026
- Amyloid-like albumin interface uncouples phagocytosis from inflammation through protein corona remodeling.Journal of colloid and interface science · 2026
- The Effect of Lactoferrin and Magnesium Phosphate Hydrogel Coating on Osteoblast Activity on Titanium Discs: An In Vitro Study.Cureus · 2026