Surface Microhardness of Enamel Exposed to Supplemented and Unsupplemented Artificial Saliva Formulations In Vitro.
Aslı Silkü Oflioğlu, Hülya Erten Can, Sude Eylül Ulucan, Ulaş Baysan, Hanife Altınışık, Shakhrukh Abdukadirov
Department of Restorative Dentistry, Faculty of Dentistry, Dokuz Eylül University, Izmir 35340, Türkiye. · Science and Technology Application and Research Center, Dokuz Eylül University, Izmir 35390, Türkiye.
Key points
From the paper's conclusion- These results describe surface mechanical responses of specific formulations at unequal doses under prolonged laboratory exposure.
Abstract
This in vitro study compared enamel surface microhardness responses to sodium fluoride (NaF), tricalcium phosphate (TCP), and calcium glycerophosphate (CaGP) in an olive leaf extract-containing artificial saliva carrier and to the unsupplemented carrier. A total of 131 human premolars were randomly allocated to NaF (n = 40), TCP (n = 40), CaGP (n = 40), or carrier (n = 11). After 96 h of demineralization, specimens underwent continuous immersion for 28 days. The primary outcome was surface microhardness recovery (ΔVHN), calculated as post-treatment minus post-demineralization Vickers hardness number (VHN). Scanning electron microscopy with energy-dispersive X-ray spectroscopy (SEM-EDX) was exploratory (n = 14). Surface hardness increased in all groups. Mean ΔVHN was 105.00 ± 53.00, 138.11 ± 50.40, 102.81 ± 48.46, and 116.98 ± 39.71 for NaF, TCP, CaGP, and carrier, respectively. The TCP formulation showed greater ΔVHN than the NaF and CaGP formulations (Bonferroni-adjusted p = 0.027 and 0.009), but no supplemented formulation showed significantly greater recovery than the carrier after multiplicity correction. Supplementary analysis likewise did not demonstrate a TCP-carrier difference (adjusted p = 0.117). No corrected SEM-EDX stage contrast was significant. These results describe surface mechanical responses of specific formulations at unequal doses under prolonged laboratory exposure. They do not establish incremental benefit over the calcium/phosphate-containing carrier or superior remineralizing efficacy of TCP; complete lesion repair cannot be inferred.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of 38% ammonia-free silver fluoride solution, with and without potassium iodide, on surface microhardness loss: An in vitro study.Archives of oral biology · 2026
- Remineralization of early caries lesions by calcium hypophosphite in vitro: a surface microhardness studyBDJ Open · 2026
- The in vitro assessment of enamel remineralization and cytotoxicity of experimental silver diamine fluoride.Biomaterial investigations in dentistry · 2026
- Biomimetic Strategies for Subsurface Enamel Remineralization: Depth-Dependent Effects of Biomimetic Agents Compared with Fluoride.Biomimetics (Basel, Switzerland) · 2026
- Remineralizing Effects of 38% Silver Diamine Fluoride and 5% Sodium Fluoride Varnish on Artificial Dentin Caries Lesions in Primary Molars: An In Vitro Study.Dentistry journal · 2026
- Comparative Remineralization Efficacy of Different Physical Forms of Chitosan in a Newly Developed Olive Leaf Extract-Containing Artificial Saliva.Molecules (Basel, Switzerland) · 2026