Material Properties and Cellular Toxicity of 3D Scaffolds Based on Poly(ester-urethane) and Titania/Titanate Nanotubes.
Dulce María González-García, Lucía Téllez-Jurado, Rodrigo Navarro Crespo, Alejandra Rubio Hernández-Sampelayo, María Rosa Aguilar, Rosa A Ramírez, Ángel Marcos Fernández
Depto. Ing. en Metalurgia y Materiales, Escuela Superior de Ingeniería Química e Industrias Extractivas (ESIQIE), Instituto Politécnico Nacional, (Unidad Profesional Adolfo López Mateos) UPALM-Zacatenco, Col. Lindavista, Mexico City 07738, Mexico. · Institute of Polymer Science and Technology (ICTP-CSIC), Juan de la Cierva, 3, 28006 Madrid, Spain.
Key points
From the paper's conclusion- In this work, scaffolds with three-dimensional structures based on poly (ester-urethane) and a mixture of titania and titanate nanotube (TNT) composites (1, 5, and 10 wt.% of nanotubes) were obtained.
Abstract
The literature on techniques for creating 3D scaffolds in tissue engineering (TE) includes methods such as electrospinning, solvent casting, freeze-drying, salt leaching, and 3D printing, among others. These techniques, used individually or in combination, produce suitable scaffolds from different materials for the reconstruction of damaged tissues. The search for materials that fulfill the function of the tissues to be reconstructed makes the design, development, and evaluation of their physicochemical properties a relevant topic of study in tissue engineering. In this work, scaffolds with three-dimensional structures based on poly (ester-urethane) and a mixture of titania and titanate nanotube (TNT) composites (1, 5, and 10 wt.% of nanotubes) were obtained. The materials showed characteristic bands due to both polymeric and titania/titanate phases (observed by Raman and FT-IR spectroscopy). Scanning Electron Microscopy (SEM) analysis showed irregular porosity with pore sizes ranging from 8 to 700 µm. Also, mechanical testing showed tensile strength values of 3.3 to 5.31 MPa and Young's modulus values of 18 to 28.8 MPa. The scaffolds were produced by a combination of freeze-drying followed by salt leaching techniques. In vitro biological assays using human osteoblast-like cells demonstrated that the materials were non-cytotoxic and supported cell viability, with excellent cell attachment and thermal stability for their intended application in tissue regeneration.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Fabrication and Characterization of a Trans-Activator of Transcription Peptide-Functionalized Collagen-Mineral Trioxide Aggregate Nanofiber Scaffold: Physicochemical Properties and Fibroblast Response.Clinical and experimental dental research · 2026
- A standardized integrated workflow to generate cellularized and decellularized silk fibroin scaffolds for bone tissue engineeringFrontiers in Bioengineering and Biotechnology · 2026
- Microbubble-Assisted Bioresorbable Biphasic Scaffolds Reinforced with TiO2 Nanosheets for Oral and Maxillofacial Bone Repair: In Vitro Evaluation.ACS omega · 2026
- Nonwoven nanofibrous PLA/SiO₂ -gelatin/hydroxyapatite hybrid scaffolds by two-nozzle electrospinning: bone tissue engineering applicationsBiomedical Materials · 2026
- HAp/PLGA/Chitosan Scaffolds Fabricated by Freeze-Drying and 3D Printing for Bone Regeneration: In Vitro Evaluation and Finite Element Analysis.Biomimetics (Basel, Switzerland) · 2026
- Fabrication and Characterization of Bioengineered Sandwich Model Scaffold for Urethral Stricture Reconstruction.Journal of biomedical materials research. Part A · 2026