Journal of Composites ScienceOpen accessMetakaolin

Optimization of Metakaolin-Based Geopolymer Composite for Repair Application

La Choviya Hawa, Abdulkader El‐Mir, Jamal Khatib, Dana Nasr, Joseph J. Assaad, Adel Elkordi, Mohamad Ezzedine El Dandachy

Beirut Arab University · University of Balamand

Key points

From the paper's conclusion
  • The Taguchi optimization method revealed that the mix design featuring A/M of 1.4, SS/SH of 2, 16 M sodium hydroxide, and curing at 60 °C yielded notable improvements in compressive and bond strengths compared to conventional cement-based composites.

Abstract

This paper assesses the feasibility of metakaolin (MK)-based geopolymer (GP) composite as an environmentally friendly substitute for cement-based composite in repair applications. The Taguchi orthogonal array method was used to find the optimum GP mix in terms of mechanical properties and adhesion to concrete substrates. Four key parameters, each with three levels, are investigated including the alkaline activator-to-MK ratio (A/M: 1, 1.2, 1.4), the sodium silicate-to-sodium hydroxide ratio (S/H: 2.0, 2.5, 3.0), sodium hydroxide (SH) molarity (12, 14, 16), and curing temperature (30, 45, 60 °C). The evaluated properties include flowability, compressive strength, splitting tensile strength, flexural strength, ultrasonic pulse velocity, and bond strength under various interface configurations. Experimental results demonstrated that the performance of MK-based GP composite was primarily governed by the A/M ratio and sodium hydroxide molarity. The Taguchi optimization method revealed that the mix design featuring A/M of 1.4, SS/SH of 2, 16 M sodium hydroxide, and curing at 60 °C yielded notable improvements in compressive and bond strengths compared to conventional cement-based composites.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers