  • From an environmental and economic perspective, plain AAC has a 50% lower embodied carbon per unit ultimate load capacity than conventional concrete.

Abstract

Low-carbon structural materials must be evaluated for mechanical performance, post-damage repair, and environmental and economic consequences. This study examined the flexural behavior, CFRP rehabilitation performance, and environmental and economic impacts of fiber-reinforced alkali-activated concrete (AAC) beams using experimental testing and nonlinear numerical models. Five sets of 15 reinforced rectangular beams (150 × 250 × 1500 mm) were tested: regular concrete, plain AAC, steel-fiber-reinforced AAC, polypropylene-fiber-reinforced AAC, and hybrid steel–polypropylene-fiber-reinforced AAC. The alkali-activated binder was 50% fly ash and 50% ground granulated blast-furnace slag. The fiber-reinforced mixtures had a fiber volume of 0.75%. Each material property assessment included three specimens per combination. All beams were four-point bent to failure, repaired using externally bonded CFRP sheets, and retested. Experimental data verified a nonlinear finite-element model produced in ANSYS APDL, which was used to explore the impact of increasing fiber content from 0.75% to 1.25%. A comparative life-cycle environmental and economic study included material production, production-associated energy, and CFRP restoration. AAC with steel-fiber reinforcement demonstrated 15.4% higher compressive, flexural, and ultimate load capacities (106.96 kN) than conventional concrete. Flexural toughness was highest in hybrid-fiber reinforcement (2406.7 kN·mm), 58.3% greater than typical concrete. Polypropylene-fiber-reinforced AAC had the best strength-recovery ratio (89.57%) and steel-fiber-reinforced AAC had the highest load capacity (84.78 kN) for CFRP rehabilitation. The numerical model projected ultimate loads that differed by 0.56% and 6.02% from the experimental values. When fiber percentage was raised to 1.25%, the steel, polypropylene, and hybrid-fiber systems’ predicted capacities improved by 25.10, 21.19, and 30.04%, respectively. From an environmental and economic perspective, plain AAC has a 50% lower embodied carbon per unit ultimate load capacity than conventional concrete. The estimated material cost was reduced by 60.7% when using fly ash.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers