Scale-Dependent Energy Dissipation in Fibre-Reinforced Concrete Beams Subjected to Low-Cycle Fatigue
Federico Accornero, Bernardino Chiaia
Key points
From the paper's conclusion- In this framework, a parametric study on beams of different depths shows, for the first time, that an optimum value of the reinforcement brittleness number, NP,opt ≈ 0.4, can be identified for the beam depths of 10 and 20 cm, which exhibit a clearly defined maximum of the energy dissipated in the first hysteretic loop, whereas no clear optimum is found for the smallest beam (5 cm), whose dissipate
Abstract
The fracturing process in fibre-reinforced brittle-matrix composites subjected to monotonic loading or low-cycle fatigue is strongly affected by the matrix damage mechanism together with the bridging action of the reinforcing fibres, including their plastic shake-down and hysteresis. The monotonic response is also considered, since it represents the envelope of the cyclic response and defines the critical (minimum reinforcement) condition against which the cyclic energy dissipation is assessed. The main features of the structural behaviour in both scenarios are associated with the fibre-reinforcement brittleness number (NP,f), which takes into account the influence of both structural size-scale and fibre volume fraction. In the case of monotonic loading, the brittleness number governs the post-cracking behaviour of the composite in terms of structural stability, which can range from ductile to catastrophic. On the other hand, when cyclic loading is considered, the brittleness number affects the cyclic energy dissipation, defined as the area enclosed by a single hysteretic loop in the load vs. deflection diagram. In the present work, numerical predictions are compared with experimental results, focusing on the evaluation of the hysteretic loops occurring in the structural behaviour of fibre-reinforced concrete beams. In this framework, a parametric study on beams of different depths shows, for the first time, that an optimum value of the reinforcement brittleness number, NP,opt ≈ 0.4, can be identified for the beam depths of 10 and 20 cm, which exhibit a clearly defined maximum of the energy dissipated in the first hysteretic loop, whereas no clear optimum is found for the smallest beam (5 cm), whose dissipated energy is almost insensitive to the brittleness number. This optimum lies below the critical value NPC ≈ 0.7 that governs the ductile-to-brittle transition under monotonic loading. On this basis, the interval NP,opt ≤ NP,f ≤ NPC is proposed as a preliminary criterion for selecting the fibre content of FRC members required to dissipate energy, e.g., under seismic actions. Since the brittleness number already accounts for the structural size, the same optimum value is found for both these beam depths, whereas the corresponding fibre volume fraction decreases with the beam depth.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Multiple Time‐Scale Homogenization of Coupled Corrosion‐Fatigue in Structural ConcreteInternational Journal for Numerical Methods in Engineering · 2026
- Concrete fatigue propagation from material to structure: Multiscale validation of a thermodynamically based discrete model on prisms and prestressed beamsEngineering Fracture Mechanics · 2026
- Fatigue Damage in Cement-Based Materials: A Critical Multiscale ReviewBuildings · 2026
- Notch depth‐dependent flexural behavior of high‐performance fiber‐reinforced concrete under static and cyclic loadingStructural Concrete · 2025
- The rate-dependent fiber-matrix interface in ultra high-performance fiber reinforced concrete: Interface property determinationCement and Concrete Composites · 2025
- Fatigue life enhancement of fibre-reinforced composites: A state-of-the-art review and outlookResults in Engineering · 2025