From the paper's conclusion
  • Coupled exposure is generally more damaging than either factor alone: alternating UV-moisture reduced the compressive strength of an glass fibre/SC-15 epoxy laminate by 30% compared to 22% under UV alone; cyclic UV–moisture exposure caused the largest transverse tensile loss (29%) in carbon/epoxy laminates; and four weeks of accelerated UV aging produced losses similar to 32 weeks of tropical outd

Abstract

Fiber-reinforced polymer composites (FRPCs) used outdoors are simultaneously exposed to ultraviolet (UV) radiation, moisture, and elevated temperatures, yet these factors are usually studied separately. This review examines UV, hygrothermal and coupled UV-hygrothermal aging of FRPCs, linking degradation mechanisms to microstructural damage and mechanical property loss. UV aging is largely confined to a thin surface layer and proceeds as photo-oxidation, chain scission, and then microcracking, whereas hygrothermal aging acts through the bulk as moisture diffusion, plasticization, hydrolysis, and fiber-matrix debonding. Coupled exposure is generally more damaging than either factor alone: alternating UV-moisture reduced the compressive strength of an glass fibre/SC-15 epoxy laminate by 30% compared to 22% under UV alone; cyclic UV–moisture exposure caused the largest transverse tensile loss (29%) in carbon/epoxy laminates; and four weeks of accelerated UV aging produced losses similar to 32 weeks of tropical outdoor exposure. In contrast to earlier reviews, coupled studies are classified here by their exposure sequences (sequential, alternating/cyclic, simultaneous and natural weathering), while conflicting results between studies are explained in terms of the fiber type, sizing, aging medium, and temperature relative to the glass transition temperature, and a minimum reporting framework for coupled aging experiments is proposed. Moisture-first exposure, field validation of accelerated tests, and physics-based service-life models remain the main research gaps.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers