  • By correlating the local strain energy distribution at the notch root with the global failure response, the results demonstrate that the calibrated ASED criterion provides highly accurate fracture load predictions across all tested materials.

Abstract

This study evaluates a calibrated Average Strain Energy Density (ASED) criterion for predicting fracture loads in additively manufactured PEEK and reinforced PEEK composites. Although the ASED criterion is a robust tool for linear-elastic materials, PEEK specimens produced via fused filament fabrication (FFF) exhibit a non-linear behavior that requires a modified approach. This work proposes a calibration of the ASED parameters (the critical strain energy and the control volume radius) to extend the applicability of this criterion to high-performance polymers with non-linear elastic response. The methodology was validated using neat PEEK and reinforced PEEK filaments: carbon-fiber reinforced (10 wt.% and 20 wt.%) and glass-fiber reinforced (20 wt.%). Experimental testing involved single-edge-notched bending (SENB) specimens with varying raster orientations (0/90, 30/−60, and 45/−45) and U-notch radii (0.00 mm—crack-like—0.25 mm, 0.50 mm, 1.00 mm, and 2.00 mm). By correlating the local strain energy distribution at the notch root with the global failure response, the results demonstrate that the calibrated ASED criterion provides highly accurate fracture load predictions across all tested materials. This research offers a reliable structural integrity assessment tool for 3D-printed PEEK components, accounting for the complex interaction between material non-linearity and notch effect, extending previous works on additive manufacturing ABS, PLA, and ASA polymers.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Extending a Calibrated Average Strain Energy Density (ASED) Criterion for Fracture Load Prediction in Notched 3D-Printed PEEK and Its Fiber-Reinforced Composites — Science Skim