International journal of molecular sciences

Polysaccharide-Modified Gold Nanoparticles: Synthesis, Catalytic and Biological Properties.

Eliza I Alibaeva, Guzel U Gil'fanova, Rinat R Gubaidullin, Ekaterina S Mescheryakova, Leonard M Khalilov, Alina D Tsvetkova, Semen N Sergeev, Nikita V Penkov,

Institute of Petrochemistry and Catalysis, Ufa Federal Research Center, Russian Academy of Sciences, Prospekt Oktyabrya 141, Ufa 450075, Russia. · Department of Materials Science and Physics of Metals, Institute of Technology and Materials, Ufa University of Science and Technology, 12 Karl Marx Street, Ufa 450008, Russia.

Key points

From the paper's conclusion
  • These results show that the properties of the resulting AuNP depend on the nature of the sulfur-modified polysaccharide used in their synthesis.

Abstract

Gold nanoparticles (AuNP) stabilized by sulfur-modified polysaccharides are of interest as multifunctional materials combining colloidal and catalytic properties, yet the influence of the polysaccharide backbone structure on nanoparticle composition and downstream bioactivity remains insufficiently understood. This study reports the synthesis of AuNP using a novel SH derivative of heparin (Hep-SH), and its comparison with previously described thiolated alginate and hyaluronic acid analogs. Reaction of Hep-SH with HAuCl4 afforded stable Hep-AuNP, confirmed by a surface plasmon resonance band at 566 nm, a spherical bimodal particle morphology (37 ± 12 and 113 ± 12 nm fractions) with a polysaccharide shell of 8-25 nm observed via SEM/BF-STEM, and colloidal stability over 14 days observed via PCCS. XPS revealed coexisting Au0/Au1+ species, and NMR spectroscopy indicated oxidation of the thiol group to a sulfonate moiety; a high negative ζ-potential (-44.7 ± 3.8 mV) is consistent with electrostatic stabilization by the polyanionic heparin shell. All three polysaccharide-modified AuNP (PS-AuNP) catalyzed the model A3-coupling reaction in a 98-99% yield at 100 °C after 8 h, whereas under milder conditions (60 °C, 4 h) the yields ranged from 25 ± 3% to 38 ± 4%, with HA-AuNP giving a significantly higher yield than Hep-AuNP and AA-AuNP. Biological evaluation on HEK293T and MDA-MB-231 cells showed that PS-AuNP caused concentration-dependent decreases in viability, which were least pronounced for HA-AuNP. These results show that the properties of the resulting AuNP depend on the nature of the sulfur-modified polysaccharide used in their synthesis. The proposed synthetic approach and the obtained materials may serve as a basis for the development of new catalysts and materials for biomedical applications.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers