Nano-SiO2/Polymer Composite Gel Fluid-Loss Reducer for High-Temperature, Salt-Resistant Water-Based Drilling Fluids: Performance and Mechanism.
Luman Liu, Jingping Liu, Yuan Geng, Ren Wang, Beiqiao Meng, Shifeng Gao, He Li, Zhe Xu,
CNPC Engineering Technology R&D Co. Ltd., Beijing 102206, China. · School of Petroleum Engineering, China University of Petroleum-East China (UPC), Qingdao 266580, China.
Key points
From the paper's conclusion- These results demonstrate the potential of SiO2@P-DAS as a nanocomposite gel fluid-loss reducer for high-temperature and salt-contaminated water-based drilling fluids.
Abstract
Polymeric gel fluid-loss reducers for water-based drilling fluids often undergo performance deterioration under combined high-temperature and high-salinity conditions. In this study, an organic-inorganic nanocomposite gel fluid-loss reducer, SiO2@P-DAS, was synthesized through aqueous free-radical polymerization using N,N-dimethylacrylamide, 2-acrylamido-2-methylpropane sulfonic acid, sodium styrene sulfonate, and KH-570-modified nano-SiO2. The corresponding polymer gel without nano-SiO2, P-DAS, was used as the control. FTIR results were consistent with the presence of modified nano-SiO2 in the composite gel. Thermogravimetric analysis showed that its initial decomposition temperature increased from 245 °C for P-DAS to 252 °C for SiO2@P-DAS. At a concentration of 3.0 wt%, the post-aging API filtrate volume of SiO2@P-DAS was 3.8 mL, compared with 4.8 mL for P-DAS after aging at 220 °C for 16 h. Under HTHP conditions of 220 °C and 3.5 MPa, the corresponding filtrate volumes were 33.33 and 49.67 mL, respectively. SiO2@P-DAS also maintained lower fluid loss under NaCl and CaCl2 contamination. At 5 wt% CaCl2, its post-aging API filtrate volume was 6.8 mL, 58.0% lower than that of P-DAS. In weighted drilling fluids with densities of 1.4-2.0 g/cm3, the post-aging API and HTHP filtrate volumes remained within 2.4-3.2 and 24.6-26.2 mL, respectively. Zeta-potential, particle-size, and filter-cake observations suggest that polymer adsorption and hydration, together with the contribution of modified nano-SiO2 to particle packing and filter-cake continuity, improve filtration control. These results demonstrate the potential of SiO2@P-DAS as a nanocomposite gel fluid-loss reducer for high-temperature and salt-contaminated water-based drilling fluids.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Molecular Screening‐Assisted Development of a Temperature‐ and Salt‐Resistant Polymeric Viscosity Reducer for Water‐Based Drilling FluidsJournal of Applied Polymer Science · 2026
- Construction and synergistic mechanism of self‐assembled nano‐unit clean fracturing fluid systemThe Canadian Journal of Chemical Engineering · 2026
- A Novel Ultrahigh-Temperature-Resistant and Multivalent-Cation-Tolerant Filtrate Reducer Based on Polysilane for Water-Based Drilling FluidsSPE Journal · 2026
- Coral‐Like Nanomaterials for Plugging Shale Microfractures in Water‐Based Drilling FluidsJournal of Applied Polymer Science · 2026
- Advancements in high-temperature and environmentally friendly water-based drilling fluids for horizontal wellsPure and Applied Chemistry · 2026
- Development and functional assessment of a polymer supported nanoscale iron hybrid for sustainable enhancement of water based drilling fluids.Discover nano · 2026