Forests

Valorization of Hemp Shives Through the Production of Bio-Based Particleboards Bonded with Calcium Lignosulfonate: A Preliminary Study

Viktor Savov, Petar Antov, Georgi Ivanov, Konstantin Vasilev, Viktoria Dudeva, Alexandrina Kostadinova-Slaveva, Stoyko Petrin

Key points

From the paper's conclusion
  • This study evaluated single-layer hemp-shive particleboards bonded solely with calcium lignosulfonate at loadings of 20%–40% dry binder solids relative to the total dry mass of the hemp–binder mixture.

Abstract

Calcium lignosulfonate offers a bio-based binder route for converting hemp shives into particleboards, but the balance between bending performance and moisture resistance requires further investigation. This study evaluated single-layer hemp-shive particleboards bonded solely with calcium lignosulfonate at loadings of 20%–40% dry binder solids relative to the total dry mass of the hemp–binder mixture. One board per formulation was hot-pressed at 180 °C, and a urea–formaldehyde-bonded board manufactured under a different pressing schedule served as a binder–process reference. Board density, 24 h water absorption and thickness swelling, and apparent bending properties were assessed. Corresponding unpressed mixtures were characterized by thermogravimetry (TG), derivative thermogravimetry (DTG), and differential scanning calorimetry (DSC) in air. Bending performance varied non-monotonically with binder content. The LS25 formulation exhibited the highest mean modulus of rupture and apparent modulus of elasticity among the lignosulfonate boards, reaching 18.49 and 3227 N·mm−2, respectively. Across the 20%–40% binder series, mean water absorption decreased from 150.7% to 55%, while thickness swelling decreased from 85.03% to 28.2%. These reductions indicate improved immersion response, although substantial moisture sensitivity remained. The unpressed mixtures lost 12.10%–24.33% of their initial mass by 150 °C and exhibited principal derivative mass-loss maxima at approximately 289–305 °C. Broad DSC minima at approximately 82–122 °C coincided with the early mass-loss region but did not establish a distinct curing transition. The observed differences describe the individual boards tested. Independent board replication and tighter control of density and furnish moisture are needed to determine whether these patterns are reproducible.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers