Crystals

Cooling Rate Sensitivity of Dendritic Spacing and T-Phase Morphology in Al-Mg-Zn Alloys

Zhenyu Wu, Xuehan Lu, Lumin Gou, Jian Bao, Zhaoxi Song, Chengcheng Chen, Jianzhong Cui, Xiangjie Wang

Key points

From the paper's conclusion
  • Within the investigated cooling rate range, the 4Mg and 8Mg alloys exhibited comparable apparent sensitivities, whereas the 12Mg alloy showed a trend toward a weaker SDAS response.

Abstract

The influence of cooling rate on the solidification behavior and microstructural evolution of Al-xMg-3Zn-0.3Cu-0.1Mn-0.12Zr alloys containing 4, 8, and 12 wt.% Mg was investigated using a wedge-shaped copper mold, which provided measured cooling rates of 10–31 K s−1. Higher cooling rates refined the grains and reduced the secondary dendrite arm spacing (SDAS), producing finer and more dispersed interdendritic constituents. Power-law fitting was employed to quantify the apparent cooling rate sensitivity of SDAS. The fitted exponents were 0.415, 0.398, and 0.196 for the 4Mg, 8Mg, and 12Mg alloys, respectively. Within the investigated cooling rate range, the 4Mg and 8Mg alloys exhibited comparable apparent sensitivities, whereas the 12Mg alloy showed a trend toward a weaker SDAS response. This behavior is consistent with changes in solute-controlled coarsening in the Mg- and Zn-rich interdendritic liquid. The Mg–Zn–Cu-enriched interdendritic constituents were identified as the Mg32(Al,Zn)49-type phase. Decreasing the cooling rate promoted the coarsening and interconnection of this phase without altering the detectable major phase constitution. At comparable cooling rates, increasing Mg content resulted in higher T-phase area fractions and more interconnected morphologies.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers