Microstructural Evolution, Properties, and Precipitation Kinetics of a High-Performance Cu–Cr–Ni–Co–Si Alloy Subjected to Cryorolling and Aging
Xinglong Sun, Yanhui Gou, Jinchuan Jie, Tingju Li, Xiaoqing Wang, Jiaqing Bao
Key points
From the paper's conclusion- The combined effects of cryorolling and aging on microstructural evolution, mechanical properties and electrical conductivity were studied, and the strengthening mechanisms and precipitation kinetics were clarified.
Abstract
Cu–Cr alloys are attractive candidates for aerospace and defense applications owing to their favorable strength-conductivity combination, although the intrinsic trade-off between strength and conductivity limits their engineering application. In this study, a CuCrNiCoSi0.6 (wt.%) alloy was fabricated by vacuum melting. The combined effects of cryorolling and aging on microstructural evolution, mechanical properties and electrical conductivity were studied, and the strengthening mechanisms and precipitation kinetics were clarified. Primary Cr3Si, Ni2Si and Co2Si phases exist in the as-cast alloy. After high-temperature treatment, Ni2Si and Co2Si dissolve into the matrix, whereas Cr3Si is retained. Cryorolling (CR) exhibits a higher dislocation density compared with room temperature rolling (RTR), which refines the width of deformation bands and the thickness of twin layers. Aging induces the formation of Cr-rich domains and (Ni,Co)2Si precipitates, which pin the boundaries of deformation bands and twin layers, and maintain structural stability. The alloy obtains optimal comprehensive performance after CR 90% deformation and aging at 440 °C for 60 min, with the ultimate tensile strength, yield strength, elongation and electrical conductivity of 753.8 MPa, 687.2 MPa, 5.6% and 48.3% IACS, respectively. The main strengthening contributions come from precipitation, grain-boundary and dislocation strengthening. Precipitation kinetic equations at different aging temperatures were established, and the precipitation activation energy was determined to be 36.3 kJ/mol.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Overcoming the strength-conductivity trade-off in Cu–3Ti alloys via a pre-aging strategyJournal of Materials Research and Technology · 2026
- Pre-aging induced concurrent enhancement of mechanical properties and softening resistance performance of Cu–Ni–Co–Si alloysJournal of Materials Research and Technology · 2025
- Achieving an enhanced strength–conductivity balance through low-temperature solution treatment in Cu–Ni–Si alloysMaterials & Design · 2026
- Effect of the evolution behavior of precipitated phases during high-temperature aging on the microstructure and properties of Cu-Al-Sc alloyJournal of Alloys and Compounds · 2026
- Dual-scale precipitation hierarchical strengthening in low-solute Cu–Ni–Si–Co alloys driven by vacuum-assisted die casting and deformationJournal of Materials Research and Technology · 2026
- Unveiling the mechanism for enhanced mechanical–electrical–tribological property integration in CuCrZr/Cu laminated metallic composites via cryorolling and short-term annealingAdvanced Composites and Hybrid Materials · 2025