Crystals

Effect of Adding Mineral Wool Production Waste on Heat-Resistant Lightweight Concrete Properties

Jolanta Pranckevičienė, Ina Pundienė

Key points

From the paper's conclusion
  • This study presents the effect of partially replacing milled fireclay (3% to 12%) with mineral wool melt centrifugation waste (CWW) in lightweight refractory concrete with cenospheres (CHs).

Abstract

This study presents the effect of partially replacing milled fireclay (3% to 12%) with mineral wool melt centrifugation waste (CWW) in lightweight refractory concrete with cenospheres (CHs). We analyzed hydration heat evolution, mineral composition (XRD), density, compressive strength, apparent porosity, and shrinkage after high-temperature exposure at 800 °C, 1000 °C, and 1200 °C. Increasing the amount of CWW accelerates the exothermic reaction (EXO) in cement paste and increases the sample compressive strength after curing and drying. After high-temperature exposure at 1000 °C and 1200 °C, due to the presence of an amorphous phase and the sintering process in the sample, additional phases, such as diopside, anorthite, and gehlenite, the compressive strength values in the samples with 6% and 9% CWW grow more intensively (up to 20.2%) than in CWW-free samples. With increasing CWW amount, the porosity of samples after high-temperature exposure at 800 °C, 1000 °C and 1200 °C varies in the ranges 41.7–35%, 38.9–33.7% and 38.1–32.2%, but shrinkage of samples varies in the range 0.09–0.2%, 0.12–0.25% and 0.13–0.33%. Overall, a CWW content of 6–12% increases compressive strength for lightweight refractory concrete with a density of 1340–1380 kg/m3 after high-temperature exposure at 1200 °C. Based on the strength-to-density ratio of the samples, a CWW content of 6–9% is optimal.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Effect of Adding Mineral Wool Production Waste on Heat-Resistant Lightweight Concrete Properties — Science Skim