Thermal Oxidation of Ti-6Al-4V for Bone Implants: A Narrow Temperature–Time Window Minimises Ti, Al and V Release in Accelerated Hydrochloric Acid Testing

Marzhan Sadenova, Lyudmila Shushkevich, Bagdat Azamatov, Boris Syrnev, Aidar Sadibekov, Sergey Gert, Amangeldi Sagidugumar

Key points

From the paper's conclusion
  • This study aimed to identify an air thermal-oxidation regime that makes the Ti-6Al-4V surface resistant to a severe acid challenge.

Abstract

Peri-implant acidification during inflammation can break down the passive film of titanium implants and release Ti, Al and, in particular, V from Ti-6Al-4V. This study aimed to identify an air thermal-oxidation regime that makes the Ti-6Al-4V surface resistant to a severe acid challenge. Polished discs oxidised at 150–800 °C for 15–60 min were characterised by optical metallography, XRD and SEM/EDS and tested for 240 h in 30% HCl, with ICP-MS analysis of the spent solutions. Protection depended strongly and non-monotonically on the temperature–time combination. Oxidation at 150 °C produced only Ti2O and slightly reduced the resistance. At 650 °C for 30 min, an ordered Ti6O layer (30.0 wt.%) with incipient rutile (1.3 wt.%) formed, the mass loss fell below the gravimetric detection limit, and dissolved Ti, Al and V decreased from 674, 52 and 32 mg L−1 to 1, 1.5 and 0.29 mg L−1. At 750 °C, the rutile content increased to about 20 wt.%, but the boundary oxide network broke up into Al- and V-rich islands and only 15–18% protection was retained. Protection was therefore governed by the continuity and chemical uniformity of the oxide layer rather than by the amount of rutile formed. These accelerated-test results require confirmation in simulated body fluids and biological studies.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers