Key points
From the paper's conclusion- This study investigates the microstructure and corrosion behaviour (simulated body fluid, 37 °C) of LPBF and wrought Ti-6Al-4V after laser surface melting (LSM) treatment.
Abstract
Ti-6Al-4V, a popular biomedical alloy, is increasingly fabricated by additive manufacturing methods, like laser powder bed fusion (LPBF). However, rapid thermal cycling and steep temperature gradients often induce mechanical degradation, corrosion, and wear. To address these challenges, laser surface modification is explored. This study investigates the microstructure and corrosion behaviour (simulated body fluid, 37 °C) of LPBF and wrought Ti-6Al-4V after laser surface melting (LSM) treatment. LSM produced modified layers of 1250–1350 µm (LPBF) and 1530–1600 µm (wrought), with gradients from remelted dendrites to acicular martensite. Microhardness in the layers increased to 655–680 HV due to lattice expansion, crystallite refinement, and higher dislocation density. However, LSM-treated alloys showed higher corrosion rates and weaker passive films, attributed to increased surface roughness, martensite formation, residual stresses, and microstructural inhomogeneity. Aluminium silicate surface films/residues further compromised passivity. Nevertheless, both LSM-LPBF and LSM-wrought specimens displayed low corrosion current densities (10−4 mA/cm2), true passivity (10−3–10−4 mA/cm2), and high resistance to localised corrosion. After cyclic polarisation, rutile-rich TiO2 surface films with aluminium silicate hydrates were observed. LSM-LPBF specimens showed slightly inferior general corrosion resistance compared to LSM-wrought counterparts, due to pronounced surface texture variations, phase/composition differences, higher microstrains and dislocation density.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Tailoring corrosion resistance of laser powder bed fusion produced Ti-6Al-4V via heat treatment at 700 °C in potential biomedical applications: Microstructural evolution and electrochemical behaviorMetals Advances · 2026
- Effects of Sandblasting at Different Angles Combined with Subsequent Acid Pickling on the Microstructure and Surface Properties of SLM-Formed Ti-6Al-4V Alloy.Micromachines · 2026
- Effect of process parameters on surface integrity in laser powder bed fusion of Ti-6Al-4V alloyScientific Reports · 2025
- Distortion Behavior of Ti6Al4V and Inconel 718 LPBF Cantilever Specimens: Effects of Scan Strategy and Stress-Relief Heat Treatment.Micromachines · 2026
- Microstructure and Corrosion Resistance of Selective Laser-Melted TC4 AlloyCrystals · 2026
- Corrosion Properties of Wrought Ti-6Al-4V and SLMed Ti-6Al-4V in 0.05 mol/L H2SO4: A Comparison InvestigationMetals · 2026